{"status":"ok","message-type":"work","message-version":"1.0.0","message":{"indexed":{"date-parts":[[2026,2,5]],"date-time":"2026-02-05T19:55:46Z","timestamp":1770321346277,"version":"3.49.0"},"reference-count":0,"publisher":"Wiley","issue":"9","license":[{"start":{"date-parts":[[2010,6,10]],"date-time":"2010-06-10T00:00:00Z","timestamp":1276128000000},"content-version":"vor","delay-in-days":0,"URL":"http:\/\/onlinelibrary.wiley.com\/termsAndConditions#vor"}],"content-domain":{"domain":[],"crossmark-restriction":false},"short-container-title":["Phys. Status Solidi (c)"],"published-print":{"date-parts":[[2010,9]]},"abstract":"<jats:title>Abstract<\/jats:title><jats:p>A Raman spectroscopy study of doped versus undoped ZnO layers is presented. The layers were grown by RF magnetron sputtering and the doping with Al, Sb and Mn was achieved by ion implantation with subsequent annealing. First\u2010order Raman response measured under \u03bb=488 nm excitation is discussed. It is shown that doping with any of the impurities used in this work produces a strong enhancement of the longitudinal optical (LO) phonon band, which is attributed to the intra\u2010band Fr\u00f6hlich mechanism. In addition, doping with Mn results in an extra mode located at 530 cm<jats:sup>\u20101<\/jats:sup>, tentatively attributed to a local vibrational mode of Mn substituting Zn in the lattice sites. (\u00a9 2010 WILEY\u2010VCH Verlag GmbH &amp; Co. KGaA, Weinheim)<\/jats:p>","DOI":"10.1002\/pssc.200983747","type":"journal-article","created":{"date-parts":[[2010,6,10]],"date-time":"2010-06-10T12:02:47Z","timestamp":1276171367000},"page":"2290-2293","source":"Crossref","is-referenced-by-count":19,"title":["Raman study of doped\u2010ZnO thin films grown by rf sputtering"],"prefix":"10.1002","volume":"7","author":[{"given":"M. F.","family":"Cerqueira","sequence":"first","affiliation":[]},{"given":"A. G.","family":"Rolo","sequence":"additional","affiliation":[]},{"given":"T.","family":"Viseu","sequence":"additional","affiliation":[]},{"given":"J.","family":"Ayres de Campos","sequence":"additional","affiliation":[]},{"given":"T.","family":"de Lacerda\u2010Ar\u00f4so","sequence":"additional","affiliation":[]},{"given":"F.","family":"Oliveira","sequence":"additional","affiliation":[]},{"given":"M. I.","family":"Vasilevskiy","sequence":"additional","affiliation":[]},{"given":"E.","family":"Alves","sequence":"additional","affiliation":[]}],"member":"311","published-online":{"date-parts":[[2010,6,10]]},"container-title":["physica status solidi c"],"original-title":[],"language":"en","link":[{"URL":"https:\/\/api.wiley.com\/onlinelibrary\/tdm\/v1\/articles\/10.1002%2Fpssc.200983747","content-type":"unspecified","content-version":"vor","intended-application":"text-mining"},{"URL":"https:\/\/onlinelibrary.wiley.com\/doi\/pdf\/10.1002\/pssc.200983747","content-type":"application\/pdf","content-version":"vor","intended-application":"text-mining"},{"URL":"https:\/\/onlinelibrary.wiley.com\/doi\/pdf\/10.1002\/pssc.200983747","content-type":"unspecified","content-version":"vor","intended-application":"similarity-checking"}],"deposited":{"date-parts":[[2023,9,12]],"date-time":"2023-09-12T14:25:55Z","timestamp":1694528755000},"score":1,"resource":{"primary":{"URL":"https:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/pssc.200983747"}},"subtitle":[],"short-title":[],"issued":{"date-parts":[[2010,6,10]]},"references-count":0,"journal-issue":{"issue":"9","published-print":{"date-parts":[[2010,9]]}},"alternative-id":["10.1002\/pssc.200983747"],"URL":"https:\/\/doi.org\/10.1002\/pssc.200983747","archive":["Portico"],"relation":{},"ISSN":["1862-6351","1610-1642"],"issn-type":[{"value":"1862-6351","type":"print"},{"value":"1610-1642","type":"electronic"}],"subject":[],"published":{"date-parts":[[2010,6,10]]}}}