{"status":"ok","message-type":"work","message-version":"1.0.0","message":{"indexed":{"date-parts":[[2026,3,15]],"date-time":"2026-03-15T05:42:48Z","timestamp":1773553368071,"version":"3.50.1"},"reference-count":67,"publisher":"Springer Science and Business Media LLC","issue":"1","license":[{"start":{"date-parts":[[2023,4,12]],"date-time":"2023-04-12T00:00:00Z","timestamp":1681257600000},"content-version":"tdm","delay-in-days":0,"URL":"https:\/\/creativecommons.org\/licenses\/by\/4.0"},{"start":{"date-parts":[[2023,4,12]],"date-time":"2023-04-12T00:00:00Z","timestamp":1681257600000},"content-version":"vor","delay-in-days":0,"URL":"https:\/\/creativecommons.org\/licenses\/by\/4.0"}],"funder":[{"DOI":"10.13039\/501100006752","name":"Universidade do Porto","doi-asserted-by":"crossref","id":[{"id":"10.13039\/501100006752","id-type":"DOI","asserted-by":"crossref"}]}],"content-domain":{"domain":["link.springer.com"],"crossmark-restriction":false},"short-container-title":["Inter Metalcast"],"published-print":{"date-parts":[[2024,1]]},"abstract":"<jats:title>Abstract<\/jats:title><jats:p>This work focused on producing and characterizing high silicon cast irons (microstructural analysis, tensile properties, damping capacity, elastic properties). Moreover, it also evaluated the influence of RE alloying on damping capacity. The samples present a step-casting geometry to verify the cooling rate\u2019s impact on their microstructures and, consequently, on the mechanical properties. The high Si SGI presented a fully ferritic matrix (<jats:italic>i.e.<\/jats:italic> pearlite &lt; 5%) with uniform dispersed graphite nodules; however, those also RE alloyed showed a lower nodularity. The results show an average increase, relative to the base SGI, of 33% for tensile strength and 55% for yield strength (section thicknesses between 45 and 25 mm). A damping capacity increase was observed, reaching a maximum increase of 32% with the addition of RE. The beneficial impact lies in the possibility of increasing the damping capacity of SGI, without compromising its tensile strength, by balancing the graphite degeneration (induced by RE alloying) and strengthening the ferritic matrix (promoted by the high Si content).<\/jats:p>","DOI":"10.1007\/s40962-023-01007-8","type":"journal-article","created":{"date-parts":[[2023,4,12]],"date-time":"2023-04-12T17:02:54Z","timestamp":1681318974000},"page":"373-389","update-policy":"https:\/\/doi.org\/10.1007\/springer_crossmark_policy","source":"Crossref","is-referenced-by-count":3,"title":["Damping Behaviour of High Silicon Nodular Cast Iron"],"prefix":"10.1007","volume":"18","author":[{"ORCID":"https:\/\/orcid.org\/0000-0002-1891-2361","authenticated-orcid":false,"given":"In\u00eas","family":"Pereira","sequence":"first","affiliation":[]},{"given":"V\u00edtor","family":"Anjos","sequence":"additional","affiliation":[]},{"given":"Gorka","family":"Alonso","sequence":"additional","affiliation":[]},{"given":"Lu\u00eds Filipe","family":"Malheiros","sequence":"additional","affiliation":[]},{"given":"R\u00e1mon","family":"Suarez","sequence":"additional","affiliation":[]}],"member":"297","published-online":{"date-parts":[[2023,4,12]]},"reference":[{"key":"1007_CR1","doi-asserted-by":"publisher","first-page":"280","DOI":"10.4028\/www.scientific.net\/msf.925.280","volume":"925","author":"P Hammersberg","year":"2018","unstructured":"P. Hammersberg, K. Hamberg, H. Borgstr\u00f6m et al., Variation of tensile properties of high silicon ductile iron. Mater. Sci. Forum 925, 280\u2013287 (2018). https:\/\/doi.org\/10.4028\/www.scientific.net\/msf.925.280","journal-title":"Mater. Sci. Forum"},{"key":"1007_CR2","unstructured":"L. Bj\u00f6rkegren. Ferritic Ductile Iron with High Silicon Content. Swedish Foundry Association, Report 941028 (1994)"},{"key":"1007_CR3","unstructured":"UNI, E. 1563. Spheroidal graphite cast irons. European Standards (2012)"},{"key":"1007_CR4","doi-asserted-by":"publisher","first-page":"159","DOI":"10.1016\/j.msea.2017.09.115","volume":"708","author":"KA Kasvayee","year":"2017","unstructured":"K.A. Kasvayee, E. Ghassemali, I.L. Svensson et al., Characterization and modeling of the mechanical behaviour of high silicon ductile iron. Mater. Sci. Eng., A 708, 159\u2013170 (2017). https:\/\/doi.org\/10.1016\/j.msea.2017.09.115","journal-title":"Mater. Sci. Eng., A"},{"issue":"4","key":"1007_CR5","first-page":"343","volume":"6","author":"R Larker","year":"2009","unstructured":"R. Larker, Solution strengthened ferritic ductile Iron ISO 1083\/JS\/500-10 provides superior consistent properties in hydraulic rotators. China Foundry 6(4), 343\u2013351 (2009)","journal-title":"China Foundry"},{"issue":"2","key":"1007_CR6","doi-asserted-by":"publisher","first-page":"35","DOI":"10.1007\/bf03355580","volume":"8","author":"W Stets","year":"2014","unstructured":"W. Stets, H. L\u00f6blich, G. Gassner et al., Solution strengthened ferritic ductile cast iron properties, production and application. Inter. Metalcast 8(2), 35\u201340 (2014). https:\/\/doi.org\/10.1007\/bf03355580","journal-title":"Inter. Metalcast"},{"key":"1007_CR7","doi-asserted-by":"publisher","DOI":"10.1007\/s40962-019-00363-8","author":"W Baer","year":"2019","unstructured":"W. Baer, Chunky graphite in ferritic spheroidal graphite cast iron: formation, prevention, characterization, impact on properties: an overview. Inter. Metalcast (2019). https:\/\/doi.org\/10.1007\/s40962-019-00363-8","journal-title":"Inter. Metalcast"},{"key":"1007_CR8","unstructured":"M. Gagn\u00e9, C., Labrecque, Microstructural defects in heavy section ductile iron castings: formation and effect on properties. AFS Trans., 561-571 (2009)"},{"key":"1007_CR9","unstructured":"H. L\u00f6blich. Einfluss der Keimbildung Bedingungen auf die Entstehung von Chunky-Graphit in dickwandigem Gusseisen mit Kugelgraphit EN-GJS. Giesserei 93(6) (2006)"},{"key":"1007_CR10","unstructured":"C. Hartung, O. Knustad, K. Wardenaer. Chunky Graphite in Ductile Iron Castings \u2013 Theories and Examples, in 8th International Foundrymen Conference, Opatija, Croatia, June 5-7 (2008)"},{"issue":"1","key":"1007_CR11","doi-asserted-by":"publisher","first-page":"12","DOI":"10.1016\/j.engfailanal.2010.07.001","volume":"18","author":"M Shirani","year":"2011","unstructured":"M. Shirani, G. H\u00e4rkeg\u00e5rd, Fatigue life distribution and size effect in ductile cast iron for wind turbine components. Eng. Fail. Anal. 18(1), 12\u201324 (2011). https:\/\/doi.org\/10.1016\/j.engfailanal.2010.07.001","journal-title":"Eng. Fail. Anal."},{"key":"1007_CR12","first-page":"6000","volume":"5000","author":"H Roedter","year":"2003","unstructured":"H. Roedter, M. Gagn\u00e9, Ductile iron for heavy section windmill castings: a European experience. Europe 5000, 6000 (2003)","journal-title":"Europe"},{"key":"1007_CR13","unstructured":"R. Okunnu. High strength solution-strengthened ferritic ductile cast iron. MSc thesis on Mechanical Engineering, Aalto University School of Engineering, Finland (2015)"},{"key":"1007_CR14","unstructured":"J. Anuncia\u00e7\u00e3o, C.S. Ribeiro, J. Matos. Viabilidade de Produ\u00e7\u00e3o de um Ferro Fundido Nodular EN-GJS-600-10 em Ambiente Industrial. Revista Fundi\u00e7\u00e3o N\u00ba 295 \u2013 Associa\u00e7\u00e3o Portuguesa de Fundi\u00e7\u00e3o (2020)"},{"key":"1007_CR15","doi-asserted-by":"publisher","first-page":"803","DOI":"10.1016\/j.msea.2017.11.051","volume":"712","author":"R Gonz\u00e1lez-Mart\u00ednez","year":"2018","unstructured":"R. Gonz\u00e1lez-Mart\u00ednez, U. de la Torre, A. Ebel et al., Effects of high silicon contents on graphite morphology and room temperature mechanical properties of as-cast ferritic ductile cast irons: part II\u2014mechanical properties. Mater. Sci. Eng. A 712, 803\u2013811 (2018). https:\/\/doi.org\/10.1016\/j.msea.2017.11.051","journal-title":"Mater. Sci. Eng. A"},{"issue":"12","key":"1007_CR16","doi-asserted-by":"publisher","first-page":"1425","DOI":"10.1179\/1743284713y.0000000483","volume":"30","author":"U de La Torre","year":"2014","unstructured":"U. de La Torre, A. Loizaga, J. Lacaze et al., As cast high silicon ductile irons with optimised mechanical properties and remarkable fatigue properties. Mater. Sci. Technol. 30(12), 1425\u20131431 (2014). https:\/\/doi.org\/10.1179\/1743284713y.0000000483","journal-title":"Mater. Sci. Technol."},{"key":"1007_CR17","first-page":"401","volume":"8","author":"GNJ Gilbert","year":"1960","unstructured":"G.N.J. Gilbert, BCIRA J. 8, 401\u2013421 (1960)","journal-title":"BCIRA J."},{"key":"1007_CR18","unstructured":"H.T. Angus. Cast Iron: Physical and Engineering Properties. Elsevier (2013)"},{"issue":"5","key":"1007_CR19","doi-asserted-by":"publisher","first-page":"603","DOI":"10.1179\/1743284711y.0000000100","volume":"28","author":"J Lacaze","year":"2012","unstructured":"J. Lacaze, P. Larra\u00f1aga, I. Asenjo et al., Influence of 1 wt% addition of ni on structural and mechanical properties of ferritic ductile irons. Mater. Sci. Technol. 28(5), 603\u2013608 (2012). https:\/\/doi.org\/10.1179\/1743284711y.0000000100","journal-title":"Mater. Sci. Technol."},{"key":"1007_CR20","doi-asserted-by":"publisher","first-page":"222","DOI":"10.1016\/j.msea.2014.03.057","volume":"605","author":"A Alhussein","year":"2014","unstructured":"A. Alhussein, M. Risbet, A. Bastien et al., Influence of silicon and addition elements on the mechanical behavior of ferritic ductile cast iron. Mater. Sci. Eng., A 605, 222\u2013228 (2014). https:\/\/doi.org\/10.1016\/j.msea.2014.03.057","journal-title":"Mater. Sci. Eng., A"},{"key":"1007_CR21","unstructured":"G.K. Bousse, J. Parolini, N. Rojek, et al. Quality Requirements for General Electric Ductile Iron Castings Exceeding 10 T Used for Wind and Gas Turbine Components, in: Proceedings of the 69th World Foundry Congress (WFC '10), vol. 3, Hangzhou, China, 2010"},{"key":"1007_CR22","unstructured":"M. Gagn\u00e9, D. Argo. Heavy Section Ductile Iron Castings \u2013 Part I: Structure and Properties, in: Easwaren J. (Ed.), Int. Conf. \"Advanced Casting Technology\", ASM Int., 231-244 (1987)"},{"key":"1007_CR23","first-page":"63","volume":"237","author":"R Kallbom","year":"2005","unstructured":"R. Kallbom, K. Hamberg, L.E. Bjorkegren, Chunky graphite formation and influence on mechanical properties in ductile cast iron. Comp. Des. Cast. Improv. Nordic Project 237, 63\u201386 (2005)","journal-title":"Comp. Des. Cast. Improv. Nordic Project"},{"issue":"1","key":"1007_CR24","doi-asserted-by":"publisher","first-page":"35","DOI":"10.1007\/s11665-006-9005-z","volume":"16","author":"P Minnebo","year":"2007","unstructured":"P. Minnebo, K.F. Nilsson, D. Blagoeva, Tensile, compression and fracture properties of thick-walled ductile cast iron components. J. Mater. Eng. Perform. 16(1), 35\u201345 (2007). https:\/\/doi.org\/10.1007\/s11665-006-9005-z","journal-title":"J. Mater. Eng. Perform."},{"issue":"5","key":"1007_CR25","doi-asserted-by":"publisher","first-page":"379","DOI":"10.1111\/j.1460-2695.2009.01337.x","volume":"32","author":"A Mouruj\u00e4rvi","year":"2009","unstructured":"A. Mouruj\u00e4rvi, K. Widell, T. Saukkonen et al., Influence of chunky graphite on mechanical and fatigue properties of heavy-section cast iron. Fatigue Fract. Eng. Mater. Struct. 32(5), 379\u2013390 (2009). https:\/\/doi.org\/10.1111\/j.1460-2695.2009.01337.x","journal-title":"Fatigue Fract. Eng. Mater. Struct."},{"key":"1007_CR26","doi-asserted-by":"publisher","first-page":"122","DOI":"10.1016\/j.msea.2012.06.024","volume":"554","author":"P Ferro","year":"2012","unstructured":"P. Ferro, P. Lazzarin, F. Berto, Fatigue properties of ductile cast iron containing chunky graphite. Mater. Sci. Eng., A 554, 122\u2013128 (2012). https:\/\/doi.org\/10.1016\/j.msea.2012.06.024","journal-title":"Mater. Sci. Eng., A"},{"issue":"9","key":"1007_CR27","doi-asserted-by":"publisher","first-page":"1601","DOI":"10.1016\/j.jmatprotec.2013.03.012","volume":"213","author":"P Ferro","year":"2013","unstructured":"P. Ferro, A. Fabrizi, R. Cervo et al., Effect of inoculant containing rare earth metals and bismuth on microstructure and mechanical properties of heavy-section near-eutectic ductile iron castings. J. Mater. Process. Technol. 213(9), 1601\u20131608 (2013). https:\/\/doi.org\/10.1016\/j.jmatprotec.2013.03.012","journal-title":"J. Mater. Process. Technol."},{"key":"1007_CR28","doi-asserted-by":"publisher","first-page":"353","DOI":"10.1016\/j.matdes.2016.09.002","volume":"111","author":"E Foglio","year":"2016","unstructured":"E. Foglio, D. Lusuardi, A. Pola et al., Fatigue design of heavy section ductile irons: influence of chunky graphite. Mater. Des. 111, 353\u2013361 (2016). https:\/\/doi.org\/10.1016\/j.matdes.2016.09.002","journal-title":"Mater. Des."},{"issue":"12","key":"1007_CR29","doi-asserted-by":"publisher","first-page":"2070","DOI":"10.1002\/adem.201600256","volume":"18","author":"T Borsato","year":"2016","unstructured":"T. Borsato, P. Ferro, F. Berto et al., Mechanical and fatigue properties of heavy section solution strengthened ferritic ductile iron castings. Adv. Eng. Mater. 18(12), 2070\u20132075 (2016). https:\/\/doi.org\/10.1002\/adem.201600256","journal-title":"Adv. Eng. Mater."},{"issue":"3","key":"1007_CR30","doi-asserted-by":"publisher","first-page":"34","DOI":"10.1016\/s1006-706x(11)60034-4","volume":"18","author":"J Khalil-Allafi","year":"2011","unstructured":"J. Khalil-Allafi, B. Amin-Ahmadi, Influence of mold preheating and silicon content on microstructure and casting properties of ductile iron in permanent mold. J. Iron. Steel Res. Int. 18(3), 34\u201339 (2011). https:\/\/doi.org\/10.1016\/s1006-706x(11)60034-4","journal-title":"J. Iron. Steel Res. Int."},{"issue":"3","key":"1007_CR31","first-page":"293","volume":"55","author":"Z Glavas","year":"2016","unstructured":"Z. Glavas, A. Strkalj, A. Stojakovic, The properties of silicon alloyed ferritic ductile irons. Metalurgija 55(3), 293\u2013296 (2016)","journal-title":"Metalurgija"},{"key":"1007_CR32","first-page":"10","volume":"307","author":"LE Bjorkegren","year":"2000","unstructured":"L.E. Bjorkegren, K. Hamberg, Silicon alloyed ductile iron with excellent ductility and machinability. Hommes et Fonderie (France) 307, 10\u201320 (2000)","journal-title":"Hommes et Fonderie (France)"},{"key":"1007_CR33","doi-asserted-by":"publisher","first-page":"33","DOI":"10.1007\/s40962-016-0112-9","volume":"11","author":"E Foglio","year":"2017","unstructured":"E. Foglio, M. Gelfi, A. Pola et al., Fatigue characterization and optimization of the production process of heavy section ductile iron castings. Inter. Metalcast 11, 33\u201343 (2017). https:\/\/doi.org\/10.1007\/s40962-016-0112-9","journal-title":"Inter. Metalcast"},{"issue":"3159","key":"1007_CR34","first-page":"657","volume":"146","author":"W Fairhurst","year":"1979","unstructured":"W. Fairhurst, K. Rohrig, High-silicon nodular irons. Foundry Trade J. 146(3159), 657\u2013681 (1979)","journal-title":"Foundry Trade J."},{"key":"1007_CR35","doi-asserted-by":"publisher","first-page":"1737","DOI":"10.1016\/B978-044452787-5.00088-3","volume-title":"Shreir\u2019s Corrosion","author":"A Reynaud","year":"2010","unstructured":"A. Reynaud, Corrosion of Cast Irons (cap. 2), in Shreir\u2019s Corrosion, vol. 3, ed. by T.J.A. Richardson (Elsevier, Amsterdam, 2010), pp.1737\u20131788"},{"issue":"4","key":"1007_CR36","doi-asserted-by":"crossref","first-page":"e032","DOI":"10.3989\/revmetalm.032","volume":"50","author":"MA Arenas","year":"2014","unstructured":"M.A. Arenas, A. Niklas, A. Conde et al., Corrosion behaviour of ductile cast irons partially modified with silicon in 0.03 M NaCl. Rev. Metal. 50(4), e032 (2014)","journal-title":"Rev. Metal."},{"issue":"12","key":"1007_CR37","doi-asserted-by":"publisher","first-page":"1479","DOI":"10.1179\/1743284714y.0000000735","volume":"31","author":"P Wei\u03b2\u00df","year":"2015","unstructured":"P. Wei\u03b2\u00df, J. Brachmann, A. B\u00fchrig-Polaczek et al., Influence of nickel and cobalt on microstructure of silicon solution strengthened ductile iron. Mater. Sci. Technol. 31(12), 1479\u20131485 (2015). https:\/\/doi.org\/10.1179\/1743284714y.0000000735","journal-title":"Mater. Sci. Technol."},{"issue":"1\u20132","key":"1007_CR38","doi-asserted-by":"publisher","first-page":"225","DOI":"10.1007\/s11085-018-9875-0","volume":"91","author":"S M\u00e9ndez","year":"2019","unstructured":"S. M\u00e9ndez, M.\u00c1. Arenas, A. Niklas et al., Effect of silicon and graphite degeneration on high-temperature oxidation of ductile cast irons in open air. Oxid. Met. 91(1\u20132), 225\u2013242 (2019). https:\/\/doi.org\/10.1007\/s11085-018-9875-0","journal-title":"Oxid. Met."},{"key":"1007_CR39","unstructured":"K. Hamberg, L.E. Bj\u00f6rkegren, Z.X. Sun. Chunky Graphite in Ductile Iron, A Literature Survey. Svenska Gjuterif\u00f6reningen, 16-49 (1997)"},{"issue":"6","key":"1007_CR40","first-page":"28","volume":"93","author":"H L\u00f6blich","year":"2006","unstructured":"H. L\u00f6blich, Einfluss der Keimbildung Bedingungen auf die Entstehung von Chunky-Graphit in dickwandigem Gusseisen mit Kugelgraphit EN-GJS. Giesserei 93(6), 28\u201341 (2006)","journal-title":"Giesserei"},{"key":"1007_CR41","unstructured":"U. Petzschmann. Vermeidung von Chunky-Graphit in dickwandigen Gussst\u00fccken aus Gusseisen mit Kugelgraphit, Final report AiF-Vorhaben 16801 N, Institut f\u00fcr Gie\u00dfereitechnik, D\u00fcsseldorf (2013)"},{"key":"1007_CR42","volume-title":"Chunky Graphite in Heavy Section Ductile Iron Castings","author":"R Kallbom","year":"2006","unstructured":"R. Kallbom, Chunky Graphite in Heavy Section Ductile Iron Castings (Chalmers University of Technology, G\u00f6teborg, Sweden, Thesis for the degree of Licentiate of Engineering, 2006)"},{"key":"1007_CR43","first-page":"36","volume":"12","author":"W Maschke","year":"2015","unstructured":"W. Maschke, Chunkygrafit - sein Auftreten und seine Vermeidung. Giesserei 12, 36\u201341 (2015)","journal-title":"Giesserei"},{"key":"1007_CR44","unstructured":"H. Loblich. Einfluss der Keimbildung Bedingungen auf die Entstehung von Chunky-Graphit in dickwandigem sowie legiertem Gusseisen mit Kugelgraphit GJS, Final report AiF-Forschungsvorhaben Nr. 13696 N\/1, Bericht E-317, Institut f\u00fcr Gie\u00dfereitechnik, D\u00fcsseldorf (2005)"},{"key":"1007_CR45","doi-asserted-by":"publisher","first-page":"1159","DOI":"10.1007\/s11661-012-1592-8","volume":"44","author":"J Sertucha","year":"2013","unstructured":"J. Sertucha, J. Lacaze, S. Armendariz et al., Statistical analysis of the influence of some trace elements on chunky graphite formation in heavy section nodular iron castings. Metall. and Mater. Trans. A. 44, 1159\u20131162 (2013). https:\/\/doi.org\/10.1007\/s11661-012-1592-8","journal-title":"Metall. and Mater. Trans. A."},{"key":"1007_CR46","unstructured":"H. Borgstr\u00f6m, V. Fourlakidis. A Review of Side-Lined Chunky Graphite Phenomena, in Proceedings of 10th International Journal of Metalcasting International Symposium on the Science and Processing of Cast Iron \u2212 SPCI10, 10-13 Nov, Mar del Plata, Argentina (2014)"},{"issue":"3","key":"1007_CR47","first-page":"107","volume":"43","author":"B Prinz","year":"1991","unstructured":"B. Prinz, K.J. Reifferscheid, T. Schulze, E. Sch\u00fcrmann et al., Untersuchung von Ursachen von Graphitentartungen bei Gu\u00dfeisen mit Kugelgraphit in Form von Chunky-Graphit. Gie\u00dfereiforschung 43(3), 107\u2013115 (1991)","journal-title":"Gie\u00dfereiforschung"},{"key":"1007_CR48","first-page":"85","volume":"78","author":"SI Karsay","year":"1970","unstructured":"S.I. Karsay, E. Campomanes, Control of graphite structure in heavy ductile iron castings. Trans. AFS 78, 85\u201392 (1970)","journal-title":"Trans. AFS"},{"key":"1007_CR49","unstructured":"Giesserei-Lexikon, 18. Auflage (Fachverlag Schiele & Sch\u00f6n) GmbH, Berlin (2001)"},{"key":"1007_CR50","first-page":"245","volume":"12\u201314","author":"M Gagn\u00e9","year":"1986","unstructured":"M. Gagn\u00e9, D. Argo, Heavy section ductile iron castings part ii: formation of chunk graphite. Proc. Int. Conf. Adv. Cast. Technol. Kalamazoo, Michigan, USA 12\u201314, 245\u2013256 (1986)","journal-title":"Proc. Int. Conf. Adv. Cast. Technol. Kalamazoo, Michigan, USA"},{"key":"1007_CR51","doi-asserted-by":"publisher","first-page":"62","DOI":"10.4028\/www.scientific.net\/msf.925.62","volume":"925","author":"B Tonn","year":"2018","unstructured":"B. Tonn, J. Lacaze, S. Duwe, Degenerated graphite growth in ductile iron. Mater. Sci. Forum 925, 62\u201369 (2018). https:\/\/doi.org\/10.4028\/www.scientific.net\/msf.925.62","journal-title":"Mater. Sci. Forum"},{"key":"1007_CR52","first-page":"16","volume":"16","author":"T Thielemann","year":"1970","unstructured":"T. Thielemann, Zur Wirkung von Spurenelementen im Gusseisen mit Kugelgraphit. Gie\u00dfereitechnik 16, 16\u201324 (1970)","journal-title":"Gie\u00dfereitechnik"},{"key":"1007_CR53","first-page":"86","volume":"94","author":"HW Hoover Jr","year":"1986","unstructured":"H.W. Hoover Jr., A literature survey on degenerated graphite in heavy section ductile iron. AFS Trans. 94, 86\u2013102 (1986)","journal-title":"AFS Trans."},{"issue":"16","key":"1007_CR54","first-page":"271","volume":"15","author":"S Hasse","year":"1995","unstructured":"S. Hasse, Die Wirkung von Spurenelementen in Gusseisen mit Kugelgraphit. Gie\u00dferei-Praxis 15(16), 271\u2013278 (1995)","journal-title":"Gie\u00dferei-Praxis"},{"key":"1007_CR55","first-page":"218","volume":"57","author":"L Dekker","year":"2010","unstructured":"L. Dekker, B. Tonn, Keimbildende Wirkung von Antimon in dickwandigem GJS zur Vermeidung von Chunky-Graphit. Giesserei-Rundschau 57, 218\u2013221 (2010)","journal-title":"Giesserei-Rundschau"},{"issue":"4","key":"1007_CR56","doi-asserted-by":"publisher","first-page":"834","DOI":"10.1179\/026708309x12560332736557","volume":"27","author":"XG Diao","year":"2011","unstructured":"X.G. Diao, Z.L. Ning, F.Y. Cao et al., Effects of antimony addition and section size on formation of chunky graphite in ductile iron. Mater. Sci. Technol. 27(4), 834\u2013838 (2011). https:\/\/doi.org\/10.1179\/026708309x12560332736557","journal-title":"Mater. Sci. Technol."},{"key":"1007_CR57","unstructured":"H. Moore Wm., L. Pritsker. Influence of Antimony on Nodular Cast Iron in Various Castings Sections. Meehanite Worldwide Report nr. E. 1307"},{"key":"1007_CR58","first-page":"14","volume":"46","author":"TC Xi","year":"1985","unstructured":"T.C. Xi, J. Fargues, M. Hecht et al., Fonderie Fondeur Aujourd\u2019hui 46, 14\u201323 (1985)","journal-title":"Fonderie Fondeur Aujourd\u2019hui"},{"key":"1007_CR59","doi-asserted-by":"publisher","first-page":"803","DOI":"10.1016\/j.msea.2017.11.050","volume":"712","author":"R Gonz\u00e1lez-Mart\u00ednez","year":"2018","unstructured":"R. Gonz\u00e1lez-Mart\u00ednez, U. de Torre, A. Ebel et al., Effects of high silicon contents on graphite morphology and room temperature mechanical properties of as-cast ferritic ductile cast irons: part I\u2014microstructure. Mater. Sci. Eng. A 712, 803\u2013811 (2018). https:\/\/doi.org\/10.1016\/j.msea.2017.11.050","journal-title":"Mater. Sci. Eng. A"},{"key":"1007_CR60","unstructured":"ISO-945, Microstructure of cast irons - Part 4: Determination of nodularity in spheroidal graphite cast irons. 2015"},{"key":"1007_CR61","volume-title":"The Physical Metallurgy of Cast Iron","author":"I Minkoff","year":"1983","unstructured":"I. Minkoff, The Physical Metallurgy of Cast Iron, vol. 292 (Wiley, New York, 1983)"},{"key":"1007_CR62","doi-asserted-by":"publisher","first-page":"410","DOI":"10.1016\/s0043-1648(03)00156-x","volume":"255","author":"AR Ghaderi","year":"2003","unstructured":"A.R. Ghaderi, M. Ahmadabadi, H.M. Ghasemi, Effect of graphite morphologies on the tribological behaviour of austempered cast iron. Wear 255, 410\u2013416 (2003). https:\/\/doi.org\/10.1016\/s0043-1648(03)00156-x","journal-title":"Wear"},{"issue":"2","key":"1007_CR63","doi-asserted-by":"publisher","first-page":"61","DOI":"10.1080\/13640461.2016.1239895","volume":"30","author":"MM Ibrahim","year":"2017","unstructured":"M.M. Ibrahim, M.M. Mourad, A.A. Nofal et al., Microstructure, hot oxidation resistance and damping capacity of Al-alloyed cast Iron. Int. J. Cast Met. Res. 30(2), 61\u201369 (2017). https:\/\/doi.org\/10.1080\/13640461.2016.1239895","journal-title":"Int. J. Cast Met. Res."},{"issue":"8","key":"1007_CR64","doi-asserted-by":"publisher","first-page":"2623","DOI":"10.1007\/s11661-002-0384-y","volume":"33","author":"SC Lin","year":"2002","unstructured":"S.C. Lin, T.S. Lui, L.H. Chen et al., Effect of pearlite on the vibration-fracture behavior of spheroidal graphite cast irons under resonant conditions. Metall. and Mater. Trans. A. 33(8), 2623\u20132634 (2002)","journal-title":"Metall. and Mater. Trans. A."},{"issue":"4","key":"1007_CR65","doi-asserted-by":"publisher","first-page":"1379","DOI":"10.2320\/matertrans.45.1379","volume":"45","author":"J-M Song","year":"2004","unstructured":"J.-M. Song et al., Effects of matrix structure on the resonant vibration behavior of spheroidal graphite cast iron. Mater. Trans. 45(4), 1379\u20131382 (2004)","journal-title":"Mater. Trans."},{"key":"1007_CR66","doi-asserted-by":"publisher","first-page":"583","DOI":"10.1063\/1.1722436","volume":"27","author":"A Granato","year":"1956","unstructured":"A. Granato, K. Lucke, Theory of mechanical damping due to dislocations. J. Appl. Phys. 27, 583\u2013593 (1956)","journal-title":"J. Appl. Phys."},{"issue":"2","key":"1007_CR67","doi-asserted-by":"publisher","first-page":"81","DOI":"10.1243\/jmes_jour_1973_015_017_02","volume":"15","author":"MAO Fox","year":"1973","unstructured":"M.A.O. Fox, R.D. Adams, Correlation of the damping capacity of cast iron with its mechanical properties and microstructure. J. Mech. Eng. Sci. 15(2), 81\u201394 (1973). https:\/\/doi.org\/10.1243\/jmes_jour_1973_015_017_02","journal-title":"J. Mech. Eng. Sci."}],"container-title":["International Journal of Metalcasting"],"original-title":[],"language":"en","link":[{"URL":"https:\/\/link.springer.com\/content\/pdf\/10.1007\/s40962-023-01007-8.pdf","content-type":"application\/pdf","content-version":"vor","intended-application":"text-mining"},{"URL":"https:\/\/link.springer.com\/article\/10.1007\/s40962-023-01007-8\/fulltext.html","content-type":"text\/html","content-version":"vor","intended-application":"text-mining"},{"URL":"https:\/\/link.springer.com\/content\/pdf\/10.1007\/s40962-023-01007-8.pdf","content-type":"application\/pdf","content-version":"vor","intended-application":"similarity-checking"}],"deposited":{"date-parts":[[2024,1,12]],"date-time":"2024-01-12T19:08:12Z","timestamp":1705086492000},"score":1,"resource":{"primary":{"URL":"https:\/\/link.springer.com\/10.1007\/s40962-023-01007-8"}},"subtitle":[],"short-title":[],"issued":{"date-parts":[[2023,4,12]]},"references-count":67,"journal-issue":{"issue":"1","published-print":{"date-parts":[[2024,1]]}},"alternative-id":["1007"],"URL":"https:\/\/doi.org\/10.1007\/s40962-023-01007-8","relation":{},"ISSN":["1939-5981","2163-3193"],"issn-type":[{"value":"1939-5981","type":"print"},{"value":"2163-3193","type":"electronic"}],"subject":[],"published":{"date-parts":[[2023,4,12]]},"assertion":[{"value":"2 November 2022","order":1,"name":"received","label":"Received","group":{"name":"ArticleHistory","label":"Article History"}},{"value":"24 February 2023","order":2,"name":"accepted","label":"Accepted","group":{"name":"ArticleHistory","label":"Article History"}},{"value":"12 April 2023","order":3,"name":"first_online","label":"First Online","group":{"name":"ArticleHistory","label":"Article History"}}]}}