{"status":"ok","message-type":"work","message-version":"1.0.0","message":{"indexed":{"date-parts":[[2026,3,16]],"date-time":"2026-03-16T14:48:08Z","timestamp":1773672488644,"version":"3.50.1"},"reference-count":37,"publisher":"MDPI AG","issue":"6","license":[{"start":{"date-parts":[[2026,3,16]],"date-time":"2026-03-16T00:00:00Z","timestamp":1773619200000},"content-version":"vor","delay-in-days":0,"URL":"https:\/\/creativecommons.org\/licenses\/by\/4.0\/"}],"funder":[{"name":"Research Fund of Yunnan Vocational Institute of Energy Technology","award":["2025LG08"],"award-info":[{"award-number":["2025LG08"]}]}],"content-domain":{"domain":[],"crossmark-restriction":false},"short-container-title":["Materials"],"abstract":"<jats:p>The application of microalloying technology has significantly improved the mechanical properties, oxidation resistance, and corrosion resistance of the Sn-9Zn-xAl-series solder. The effects of Al addition on microstructural evolution and service-related performance of the solders were systematically investigated using a combination of characterization techniques, including scanning electron microscopy\/energy-dispersive X-ray spectroscopy (SEM\/EDX), differential scanning calorimetry (DSC), tensile testing, spreading testing, thermogravimetry (TG), and potentiodynamic polarization measurements. Microstructural characterization reveals that an optimal content of Al reacts with the Sn-Zn matrix to form AlZnSn intermetallic compounds (IMCs), which effectively refines the Zn-rich precipitates and eutectic lamellar structure. Concomitantly, the formation of second-phase strengthening contributes to a significant enhancement in the tensile strength of the solder alloys. Specifically, the Sn-9Zn-0.8Al solder exhibits a tensile strength of 87 MPa, corresponding to a 37% increment compared to the base Sn-9Zn alloy, whereas the elongation is reduced to 14.1%. Moreover, the in situ-formed Al2O3 passive film provides effective protection for the solder matrix, inhibiting oxidation induced by oxygen atoms and corrosion caused by chlorine ions, thereby remarkably improving the oxidation and corrosion resistance of the alloy. Collectively, these findings demonstrate that Al microalloying can substantially enhance the strength, oxidation resistance, and corrosion resistance of Sn-9Zn solder; however, a trade-off between wettability and ductility needs to be carefully considered for practical applications.<\/jats:p>","DOI":"10.3390\/ma19061159","type":"journal-article","created":{"date-parts":[[2026,3,16]],"date-time":"2026-03-16T13:32:07Z","timestamp":1773667927000},"page":"1159","update-policy":"https:\/\/doi.org\/10.3390\/mdpi_crossmark_policy","source":"Crossref","is-referenced-by-count":0,"title":["Effects of Al Element on the Microstructure and Properties of Sn-9Zn Solder Alloy"],"prefix":"10.3390","volume":"19","author":[{"given":"Jiaojiao","family":"Yang","sequence":"first","affiliation":[{"name":"Faculty of Resources and Environmental Engineering, Yunnan Vocational Institute of Energy Technology, Qujing 655001, China"},{"name":"Faculty of Materials Science and Engineering, Kunming University of Science and Technology, Kunming 650093, China"}],"role":[{"role":"author","vocabulary":"crossref"}]},{"given":"Yuanqi","family":"You","sequence":"additional","affiliation":[{"name":"Faculty of Materials Science and Engineering, Kunming University of Science and Technology, Kunming 650093, China"}],"role":[{"role":"author","vocabulary":"crossref"}]},{"given":"Gaohua","family":"Jiang","sequence":"additional","affiliation":[{"name":"Faculty of Resources and Environmental Engineering, Yunnan Vocational Institute of Energy Technology, Qujing 655001, China"}],"role":[{"role":"author","vocabulary":"crossref"}]},{"given":"Caiju","family":"Li","sequence":"additional","affiliation":[{"name":"Faculty of Materials Science and Engineering, Kunming University of Science and Technology, Kunming 650093, China"}],"role":[{"role":"author","vocabulary":"crossref"}]}],"member":"1968","published-online":{"date-parts":[[2026,3,16]]},"reference":[{"key":"ref_1","doi-asserted-by":"crossref","first-page":"4952","DOI":"10.1007\/s11664-022-09732-2","article-title":"Effects of Bi Addition on the Solderability and Mechanical Properties of Sn-Zn-Cu Lead-Free Solder","volume":"51","author":"Pu","year":"2022","journal-title":"J. Electron. Mater."},{"key":"ref_2","doi-asserted-by":"crossref","first-page":"114599","DOI":"10.1016\/j.microrel.2022.114599","article-title":"Effects of Ga alloying on microstructure and comprehensive performances of Sn\u20139Zn\u20132Bi alloys for the microelectronics industry","volume":"135","author":"Peng","year":"2022","journal-title":"Microelectron. Reliab."},{"key":"ref_3","doi-asserted-by":"crossref","first-page":"149","DOI":"10.1016\/j.jallcom.2004.08.079","article-title":"Investigations on microhardness of Sn\u2013Zn based lead-free solder alloys as replacement of Sn\u2013Pb solder","volume":"392","author":"Islam","year":"2005","journal-title":"J. Alloys Compd."},{"key":"ref_4","doi-asserted-by":"crossref","first-page":"701","DOI":"10.1007\/BF02651362","article-title":"Lead (Pb)-free solders for electronic packaging","volume":"23","author":"Kang","year":"1994","journal-title":"J. Electron. Mater."},{"key":"ref_5","doi-asserted-by":"crossref","first-page":"1253","DOI":"10.1016\/j.microrel.2014.02.025","article-title":"A review: On the development of low melting temperature Pb-free solders","volume":"54","author":"Kotadia","year":"2014","journal-title":"Microelectron. Reliab."},{"key":"ref_6","doi-asserted-by":"crossref","first-page":"9065","DOI":"10.1007\/s10854-019-01333-w","article-title":"The reliability of lead-free solder joint subjected to special environment: A review","volume":"30","author":"Wang","year":"2019","journal-title":"J. Mater. Sci. Mater. Electron."},{"key":"ref_7","doi-asserted-by":"crossref","first-page":"263","DOI":"10.1557\/JMR.2002.0036","article-title":"Effect of Cu concentration on the interfacial reactions between Ni and Sn\u2013Cu solders","volume":"17","author":"Chen","year":"2002","journal-title":"J. Mater. Res."},{"key":"ref_8","doi-asserted-by":"crossref","first-page":"277","DOI":"10.1108\/SSMT-10-2021-0064","article-title":"Development of holmium doped eutectic Sn-Ag lead-free solder for electronic packaging","volume":"34","author":"Shalaby","year":"2022","journal-title":"Solder. Surf. Mt. Technol."},{"key":"ref_9","doi-asserted-by":"crossref","first-page":"379","DOI":"10.1007\/s42114-021-00231-2","article-title":"Deformation mechanism of various Sn-xBi alloys under tensile tests","volume":"4","author":"Cai","year":"2021","journal-title":"Adv. Compos. Hybrid Mater."},{"key":"ref_10","doi-asserted-by":"crossref","first-page":"25","DOI":"10.1007\/BF03222376","article-title":"Microstructure and mechanical properties of Sn-In and Sn-Bi solders","volume":"45","author":"Morris","year":"1993","journal-title":"JOM"},{"key":"ref_11","doi-asserted-by":"crossref","first-page":"1355","DOI":"10.1007\/s11664-004-0165-z","article-title":"Effect of cooling rate on microstructure and shear strength of pure Sn, Sn-0.7 Cu, Sn-3.5 Ag, and Sn-37Pb solders","volume":"33","author":"Maveety","year":"2004","journal-title":"J. Electron. Mater."},{"key":"ref_12","doi-asserted-by":"crossref","first-page":"77","DOI":"10.1016\/j.microrel.2017.06.016","article-title":"A review of lead-free solders for electronics applications","volume":"75","author":"Cheng","year":"2017","journal-title":"Microelectron. Reliab."},{"key":"ref_13","doi-asserted-by":"crossref","first-page":"55","DOI":"10.1016\/S1359-0286(00)00036-X","article-title":"Advances in lead-free electronics soldering","volume":"5","author":"Suganuma","year":"2001","journal-title":"Curr. Opin. Solid State Mater. Sci."},{"key":"ref_14","first-page":"65","article-title":"Lead-free solders for electronic assembly: Design & reliability of solders and solder interconnections","volume":"52","author":"Hua","year":"1997","journal-title":"Proc. TMS Symp."},{"key":"ref_15","doi-asserted-by":"crossref","first-page":"1269","DOI":"10.1016\/S1359-6462(99)00302-4","article-title":"Development of fluxes for lead-free solders containing zinc","volume":"41","author":"Vaynman","year":"1999","journal-title":"Scr. Mater."},{"key":"ref_16","doi-asserted-by":"crossref","first-page":"478","DOI":"10.1016\/j.jallcom.2007.05.087","article-title":"Study on the properties of Sn\u20139Zn\u2013xCr lead-free solder","volume":"460","author":"Chen","year":"2008","journal-title":"J. Alloys Compd."},{"key":"ref_17","doi-asserted-by":"crossref","first-page":"251","DOI":"10.1016\/j.jallcom.2016.01.006","article-title":"Alloying influences on low melt temperature SnZn and SnBi solder alloys for electronic interconnections","volume":"665","author":"Ren","year":"2016","journal-title":"J. Alloys Compd."},{"key":"ref_18","doi-asserted-by":"crossref","first-page":"13914","DOI":"10.1007\/s10854-018-9524-z","article-title":"Wetting kinetics and spreading phenomena of Sn-35Bi-1Ag solder on different substrates","volume":"29","author":"Li","year":"2018","journal-title":"J. Mater. Sci. Mater. Electron."},{"key":"ref_19","doi-asserted-by":"crossref","first-page":"2297","DOI":"10.1007\/s10854-014-1875-5","article-title":"Effect of doping Al on the liquid oxidation of Sn\u2013Bi\u2013Zn solder","volume":"25","author":"Wang","year":"2014","journal-title":"J. Mater. Sci. Mater. Electron."},{"key":"ref_20","doi-asserted-by":"crossref","first-page":"515","DOI":"10.1007\/s13391-013-3087-1","article-title":"Development of extremely ductile lead-free Sn-Al solders for futuristic electronic packaging applications","volume":"10","author":"Alam","year":"2014","journal-title":"Electron. Mater. Lett."},{"key":"ref_21","doi-asserted-by":"crossref","first-page":"115753","DOI":"10.1016\/j.matchar.2025.115753","article-title":"Eliminating room-temperature brittleness via introducing residual interface defects to control element diffusion pathways","volume":"230","author":"You","year":"2025","journal-title":"Mater. Charact."},{"key":"ref_22","unstructured":"(2021). Metallic Materials\u2014Tensile Testing\u2014Part 1: Method of Test at Room Temperature (Standard No. GB\/T 228.1-2021)."},{"key":"ref_23","doi-asserted-by":"crossref","first-page":"369","DOI":"10.1007\/s10973-012-2318-2","article-title":"Phase transition temperatures of Sn\u2013Zn\u2013Al system and their comparison with calculated phase diagrams","volume":"110","author":"Smetana","year":"2012","journal-title":"J. Therm. Anal. Calorim."},{"key":"ref_24","doi-asserted-by":"crossref","first-page":"563","DOI":"10.1007\/s12613-013-0766-8","article-title":"Effects of phosphorus addition on the properties of Sn-9Zn lead-free solder alloy","volume":"20","author":"Huang","year":"2013","journal-title":"Int. J. Miner. Metall. Mater."},{"key":"ref_25","first-page":"35","article-title":"Interfacial Microstructure, Microhardness and Tensile Properties of Al Micro-Particle Doped Sn-9Zn Eutectic Pb-Free Solder Alloy for Microelectronics Applications","volume":"4","author":"Islam","year":"2012","journal-title":"J. Telecommun. Electron. Comput. Eng. JTEC"},{"key":"ref_26","doi-asserted-by":"crossref","first-page":"245","DOI":"10.1016\/j.msea.2017.06.092","article-title":"Influence of small addition of antimony (Sb) on thermal behavior, microstructural and tensile properties of Sn-9.0 Zn-0.5 Al Pb-free solder alloy","volume":"701","author":"Deghady","year":"2017","journal-title":"Mater. Sci. Eng. A"},{"key":"ref_27","unstructured":"Gupta, K.K., and Bhattamishra, S.D. (2015). Effect of Addition of Al to Sn-Zn Solder Alloys. [Bachelor Thesis, National Institute of Technology Rourkela]. Available online: http:\/\/ethesis.nitrkl.ac.in\/7016\/."},{"key":"ref_28","doi-asserted-by":"crossref","first-page":"1528","DOI":"10.1557\/JMR.2003.0211","article-title":"Microstructures and mechanical properties of Sn\u20138.55 Zn\u20130.45 Al\u2013XAg solders","volume":"18","author":"Huang","year":"2003","journal-title":"J. Mater. Res."},{"key":"ref_29","doi-asserted-by":"crossref","first-page":"317","DOI":"10.1016\/j.jallcom.2016.12.191","article-title":"Influence of Ce addition on Sn-3.0 Ag-0.5 Cu solder joints: Thermal behavior, microstructure and mechanical properties","volume":"698","author":"Tu","year":"2017","journal-title":"J. Alloys Compd."},{"key":"ref_30","doi-asserted-by":"crossref","first-page":"295","DOI":"10.1016\/j.msea.2013.10.008","article-title":"Effects of Ni-coated carbon nanotubes addition on the microstructure and mechanical properties of Sn\u2013Ag\u2013Cu solder alloys","volume":"590","author":"Yang","year":"2014","journal-title":"Mater. Sci. Eng. A"},{"key":"ref_31","doi-asserted-by":"crossref","first-page":"119","DOI":"10.1016\/j.jmst.2022.06.009","article-title":"Strengthening and deformation mechanism of high-strength CrMnFeCoNi high entropy alloy prepared by powder metallurgy","volume":"132","author":"Xing","year":"2022","journal-title":"J. Mater. Sci. Technol."},{"key":"ref_32","doi-asserted-by":"crossref","first-page":"522","DOI":"10.1002\/maco.201508605","article-title":"Understanding corrosion mechanism of Sn\u2013Zn alloys in NaCl solution via corrosion products characterization","volume":"67","author":"Liu","year":"2016","journal-title":"Mater. Corros."},{"key":"ref_33","doi-asserted-by":"crossref","first-page":"52","DOI":"10.1108\/SSMT-05-2018-0013","article-title":"Corrosion characterization of Sn-Zn solder: A review","volume":"31","author":"Yahaya","year":"2019","journal-title":"Solder. Surf. Mt. Technol."},{"key":"ref_34","doi-asserted-by":"crossref","first-page":"150","DOI":"10.1016\/j.corsci.2016.07.004","article-title":"Effects of intermetallic-forming element additions on microstructure and corrosion behavior of Sn\u2013Zn solder alloys","volume":"112","author":"Liu","year":"2016","journal-title":"Corros. Sci."},{"key":"ref_35","doi-asserted-by":"crossref","first-page":"6400","DOI":"10.1016\/j.jmrt.2023.11.123","article-title":"Effect of Ag addition on the microstructure and corrosion properties of Sn\u20139Zn lead-free solder","volume":"27","author":"Pu","year":"2023","journal-title":"J. Mater. Res. Technol."},{"key":"ref_36","doi-asserted-by":"crossref","first-page":"1539","DOI":"10.1007\/s10854-024-13277-x","article-title":"Influence of alloying elements on microstructure, mechanical properties and corrosion behaviour of hypoeutectic Sn-6.5wt%Zn-0.5 wt%X (X = Ag, Al, Cu) lead-free solders","volume":"35","author":"Figueroa","year":"2024","journal-title":"J. Mater. Sci. Mater. Electron."},{"key":"ref_37","doi-asserted-by":"crossref","first-page":"2424","DOI":"10.1016\/j.jallcom.2016.11.138","article-title":"Effect of phase composition and microstructure on the corrosion resistance of Ni-Al intermetallic compounds","volume":"695","author":"Wen","year":"2017","journal-title":"J. Alloys Compd."}],"container-title":["Materials"],"original-title":[],"language":"en","link":[{"URL":"https:\/\/www.mdpi.com\/1996-1944\/19\/6\/1159\/pdf","content-type":"unspecified","content-version":"vor","intended-application":"similarity-checking"}],"deposited":{"date-parts":[[2026,3,16]],"date-time":"2026-03-16T13:33:45Z","timestamp":1773668025000},"score":1,"resource":{"primary":{"URL":"https:\/\/www.mdpi.com\/1996-1944\/19\/6\/1159"}},"subtitle":[],"short-title":[],"issued":{"date-parts":[[2026,3,16]]},"references-count":37,"journal-issue":{"issue":"6","published-online":{"date-parts":[[2026,3]]}},"alternative-id":["ma19061159"],"URL":"https:\/\/doi.org\/10.3390\/ma19061159","relation":{},"ISSN":["1996-1944"],"issn-type":[{"value":"1996-1944","type":"electronic"}],"subject":[],"published":{"date-parts":[[2026,3,16]]}}}