{"status":"ok","message-type":"work","message-version":"1.0.0","message":{"indexed":{"date-parts":[[2026,5,1]],"date-time":"2026-05-01T11:50:52Z","timestamp":1777636252841,"version":"3.51.4"},"reference-count":46,"publisher":"MDPI AG","issue":"4","license":[{"start":{"date-parts":[[2020,4,7]],"date-time":"2020-04-07T00:00:00Z","timestamp":1586217600000},"content-version":"vor","delay-in-days":0,"URL":"https:\/\/creativecommons.org\/licenses\/by\/4.0\/"}],"funder":[{"DOI":"10.13039\/501100001871","name":"Funda\u00e7\u00e3o para a Ci\u00eancia e a Tecnologia","doi-asserted-by":"publisher","award":["PTDC\/ECI-EGC\/30681\/2017"],"award-info":[{"award-number":["PTDC\/ECI-EGC\/30681\/2017"]}],"id":[{"id":"10.13039\/501100001871","id-type":"DOI","asserted-by":"publisher"}]}],"content-domain":{"domain":[],"crossmark-restriction":false},"short-container-title":["Coatings"],"abstract":"<jats:p>Hydrophobic materials are among the most commonly used coatings for building exterior cladding. In fact, these products are easily applied to an existing surface, significantly reduce water absorption and have a minimal impact on the aesthetic properties. On the other hand, although these products have a proven effectiveness, their long-term durability to weathering has not yet been systematically studied and completely understood. For these reasons, this study aims to correlate the effect of artificial aging on the moisture transport properties of hydrophobic treatments when applied on building exterior claddings. Three hydrophobic products (an SiO2-TiO2 nanostructured dispersion; a silane\/oligomeric siloxane; and a siloxane) were applied on samples of limestone and of a cement-based mortar. The moisture transport properties (water absorption, drying, water vapor permeability) of untreated and treated specimens were characterized. Furthermore, the long-term durability of the specimens was evaluated by artificial aging, that is, hygrothermal cycles (freeze\u2013thaw and hot\u2013cold). All treatments have significant hydrophobic effectiveness and improve the long term-durability of the treated specimens. However, the results showed that the three hydrophobic products have different effectiveness and durability, with the SiO2-TiO2 nanostructured dispersion being the most durable treatment on limestone, and the siloxane the most suitable for cementitious mortar.<\/jats:p>","DOI":"10.3390\/coatings10040363","type":"journal-article","created":{"date-parts":[[2020,4,8]],"date-time":"2020-04-08T05:59:47Z","timestamp":1586325587000},"page":"363","update-policy":"https:\/\/doi.org\/10.3390\/mdpi_crossmark_policy","source":"Crossref","is-referenced-by-count":18,"title":["Effect of Hygrothermal Aging on Hydrophobic Treatments Applied to Building Exterior Claddings"],"prefix":"10.3390","volume":"10","author":[{"ORCID":"https:\/\/orcid.org\/0000-0002-2194-4620","authenticated-orcid":false,"given":"Giovanni","family":"Borsoi","sequence":"first","affiliation":[{"name":"CERIS, Civil Engineering Research and Innovation for Sustainability, Instituto Superior T\u00e9cnico, University of Lisbon, 1000-147 Lisbon, Portugal"}]},{"given":"Carlos","family":"Esteves","sequence":"additional","affiliation":[{"name":"CERIS, Civil Engineering Research and Innovation for Sustainability, Instituto Superior T\u00e9cnico, University of Lisbon, 1000-147 Lisbon, Portugal"}]},{"ORCID":"https:\/\/orcid.org\/0000-0003-4038-6748","authenticated-orcid":false,"given":"In\u00eas","family":"Flores-Colen","sequence":"additional","affiliation":[{"name":"CERIS, Civil Engineering Research and Innovation for Sustainability, Instituto Superior T\u00e9cnico, University of Lisbon, 1000-147 Lisbon, Portugal"}]},{"ORCID":"https:\/\/orcid.org\/0000-0002-7135-8603","authenticated-orcid":false,"given":"Ros\u00e1rio","family":"Veiga","sequence":"additional","affiliation":[{"name":"LNEC, National Laboratory for Civil Engineering, 1000-147 Lisbon, Portugal"}]}],"member":"1968","published-online":{"date-parts":[[2020,4,7]]},"reference":[{"key":"ref_1","unstructured":"Fassina, V. (2000). Assessment of durability of water repellents by means of exposure testes. 9th International Congress on Deterioration and Conservation of Stone, Elsevier."},{"key":"ref_2","unstructured":"Roos, M., Konig, F., Stadtmuller, S., and Weyershausen, B. (2008). Evolution of silicone based water repellents for modern building protection. 5th International Conference on Water Repellent Treatment of Building Mate-Rials\u2014Hydrophobe V, Aedificatio Publishers."},{"key":"ref_3","unstructured":"Medeiros, M. (2008). Contribui\u00e7\u00e3o ao Estudo da Durabilidade de Concretos com Protec\u00e7\u00e3o Superficial Frente \u00e0 a\u00e7\u00e3o de \u00edons Cloretos. [Ph.D. Thesis, Polytechnic School of the University of S\u00e3o Paulo]."},{"key":"ref_4","doi-asserted-by":"crossref","first-page":"39","DOI":"10.1016\/j.enbuild.2012.07.002","article-title":"Effect of moisture content on heat and moisture transport and storage properties of thermal insulation materials","volume":"53","author":"Jerman","year":"2012","journal-title":"Energ. Build."},{"key":"ref_5","doi-asserted-by":"crossref","first-page":"939","DOI":"10.1007\/s11242-011-9884-9","article-title":"Water vapor adsorption in porous building materials: Experimental measurement and theoretical analysis","volume":"91","author":"Medved","year":"2012","journal-title":"Transp. Porous Med."},{"key":"ref_6","doi-asserted-by":"crossref","first-page":"744","DOI":"10.1016\/j.cemconcomp.2009.07.002","article-title":"Water permeability of engineered cementitious composites","volume":"31","author":"Lepech","year":"2009","journal-title":"Cem. Concr. Comp."},{"key":"ref_7","doi-asserted-by":"crossref","first-page":"131","DOI":"10.1007\/978-981-10-0648-7_7","article-title":"Durability of ETICS and Premixed One-Coat Renders in Natural Exposure Conditions","volume":"Volume 6","author":"Delgado","year":"2016","journal-title":"New Approaches to Building Pathology and Durability"},{"key":"ref_8","doi-asserted-by":"crossref","first-page":"259","DOI":"10.1016\/S0950-0618(97)00046-9","article-title":"Hydrophobic treatment of concrete","volume":"11","author":"Polder","year":"1997","journal-title":"Constr. Build. Mater."},{"key":"ref_9","unstructured":"Maranh\u00e3o, F., and Loh, K. (2010). The Use of Hydrophobic Products in Porous Building Materials, T\u00e9chne Edition."},{"key":"ref_10","doi-asserted-by":"crossref","first-page":"2686","DOI":"10.1080\/15567036.2018.1511642","article-title":"Hydrophilic and hydrophobic materials and their applications","volume":"40","author":"Ahmad","year":"2018","journal-title":"Energy Sources Part A"},{"key":"ref_11","first-page":"42","article-title":"Preservation for the Future: The need for waterproofing structures above and below ground","volume":"7","author":"Edwards","year":"2002","journal-title":"J. Protect. Coat. Linings"},{"key":"ref_12","unstructured":"Finzel, W., and Vincent, H. (1996). Silicones in Coatings. Federation Series on Coatings Technology, Federation of Societies for Coatings Technology."},{"key":"ref_13","first-page":"26","article-title":"Chemical Considerations for Making Low-VOC Silicon-Based Water Repellents","volume":"7","author":"Selley","year":"2010","journal-title":"J. Coat. Technol. Res."},{"key":"ref_14","unstructured":"Charola, A. (2001). Water repellents and other \u201cprotective\u201d treatments: A critical review. 3rd International Conference on Surface Technology with Water Repellents Agents\u2014Hydrophone III, Aedificatio Publishers."},{"key":"ref_15","doi-asserted-by":"crossref","unstructured":"Alexander, M.G., Beushausen, H.D., Dehn, F., and Moyo, P. (2008). Hydrophobic treatments on concrete. Evaluation of the durability and non-destructive testing. 2nd International Conference on Concrete Repair, Rehabilitation and Retrofitting II, CRC Press.","DOI":"10.1201\/9781439828403"},{"key":"ref_16","first-page":"104","article-title":"Notch effect and fracture load predictions of rock beams at different temperatures using the Theory of Critical Distances","volume":"125","author":"Justo","year":"2020","journal-title":"Int. J. Rock Mech. Min."},{"key":"ref_17","doi-asserted-by":"crossref","first-page":"157","DOI":"10.1016\/j.conbuildmat.2015.12.181","article-title":"Study of the effect of three anti-graffiti products on the physical properties of different substrates","volume":"107","author":"Moura","year":"2016","journal-title":"Constr. Build. Mater."},{"key":"ref_18","unstructured":"CEN\u2014European Committee for Standardization (2006). Methods of Test for Mortar for Masonry\u2014Part 2: Bulk Sampling of Mortars and Preparation of Test Mortars, CEN. EN 1015-2."},{"key":"ref_19","doi-asserted-by":"crossref","first-page":"1379","DOI":"10.1007\/s11998-019-00220-7","article-title":"The influence of hydrophobic protection on building exterior claddings","volume":"16","author":"Esteves","year":"2019","journal-title":"J. Coat. Technol. Res."},{"key":"ref_20","doi-asserted-by":"crossref","first-page":"13","DOI":"10.1016\/j.ijadhadh.2018.07.008","article-title":"Investigation of hydrophobic coatings on cellulose-fiber substrates with in-situ polymerization of silane\/siloxane mixtures","volume":"86","author":"Rutter","year":"2018","journal-title":"Int. J. Adhes. Adhes."},{"key":"ref_21","doi-asserted-by":"crossref","first-page":"103","DOI":"10.1016\/j.apsusc.2015.12.116","article-title":"Surface modification to produce hydrophobic nano-silica particles using sodium dodecyl sulfate as a modifier","volume":"364","author":"Qiao","year":"2016","journal-title":"Appl. Surf. Sci."},{"key":"ref_22","doi-asserted-by":"crossref","first-page":"122","DOI":"10.1016\/j.colsurfa.2019.04.077","article-title":"Coupling of synthesis and modification to produce hydrophobic or functionalized nano-silica particles","volume":"574","author":"Yu","year":"2019","journal-title":"Colloid Surf. A"},{"key":"ref_23","doi-asserted-by":"crossref","first-page":"400","DOI":"10.1016\/j.porgcoat.2012.10.006","article-title":"TiO2\u2013SiO2\u2013PDMS nano-composite hydrophobic coating with self-cleaning properties for marble protection","volume":"76","author":"Kapridaki","year":"2013","journal-title":"Prog. Org. Coat."},{"key":"ref_24","doi-asserted-by":"crossref","first-page":"72","DOI":"10.1016\/j.buildenv.2016.10.019","article-title":"Synthesis and characterization of photocatalytic hydrophobic hybrid TiO2-SiO2 coatings for building applications","volume":"111","author":"Alfieri","year":"2017","journal-title":"Build. Environ."},{"key":"ref_25","doi-asserted-by":"crossref","unstructured":"Truppi, A., Luna, M., Petronella, F., Falcicchio, A., Giannini, C., Comparelli, R., and Mosquera, M.J. (2018). Photocatalytic activity of TiO2\/AuNRs\u2013SiO2 nanocomposites applied to building materials. Coatings, 8.","DOI":"10.3390\/coatings8090296"},{"key":"ref_26","unstructured":"CEN\u2014European Committee for Standardization (2002). Methods of Test for Mortar for Masonry\u2014Part 18: Determination of Water Absorption Coefficient due to Capillary Action of Hardened Mortar, CEN. EN 1015-18."},{"key":"ref_27","unstructured":"RILEM (1980). Water Absorption under Low Pressure, Pipe Method, Test No 11.4. Recommandations Provisoires, RILEM Publications SARL. RILEM TC 25-PEM."},{"key":"ref_28","unstructured":"RILEM (1980). Evaporation Curve, Test No 11.5, RILEM Publications SARL. Recommandations Provisoires; RILEM TC 25-PEM."},{"key":"ref_29","unstructured":"(1988). NORMAL 29\/88\u2014Misure dell\u2019Indice di Asciugamento (Drying Index), Alterazioni dei Materiali Lapidei e Trattamenti Conservative\u2014Proposte per l\u2019unificazione dei Metodi Sperimentali di Studio e Controllo, ICR-CNR."},{"key":"ref_30","unstructured":"(2008). CEN\u2014European Committee for Standardization, Methods of Test for Mortar for Masonry\u2014Part 19: Determination of Water Vapour Permeability of Hardened Rendering and Plastering Mortars, CEN. EN 1015-19."},{"key":"ref_31","unstructured":"Thompson, G. (2006). Development of Artificial Ageing Tests for Renders\u2014Application to Conservation Mortars. 7th International Masonry Conference\u20147IMC, International Masonry Society."},{"key":"ref_32","unstructured":"Ghiassi, B., and Louren\u00e7o, P. (2019). Long-term Performance and Durability of Masonry Structures Degradation Mechanisms, Health Monitoring and Service Life Design, Chapter 6\u2014Mortars, Elsevier."},{"key":"ref_33","unstructured":"(2002). CEN\u2014European Committee for Standardization, Methods of test for Mortar for Masonry\u2014Part 21: Determination of the Compatibility of One-Coat Rendering Mortars with Substrates, CEN. EN 1015-21."},{"key":"ref_34","doi-asserted-by":"crossref","first-page":"321","DOI":"10.1179\/2047058414Y.0000000151","article-title":"Consolidation and chromatic reintegration of historical renders with lime-based pozzolanic products","volume":"60","author":"Pascoal","year":"2015","journal-title":"Stud. Conser."},{"key":"ref_35","doi-asserted-by":"crossref","first-page":"112","DOI":"10.1617\/s11527-019-1411-4","article-title":"Assessment of test methods for the durability of thermal mortars exposure to freezing","volume":"52","author":"Maia","year":"2019","journal-title":"Mater. Struct."},{"key":"ref_36","unstructured":"Groot, C., Ashall, G., and Hughes, J. (2004). Porosity of historic mortars. Characterisation of Old Mortars with Respect to Their Repair\u2013Final Report of RILEM TC 167-COM, RILEM Publications SARL."},{"key":"ref_37","doi-asserted-by":"crossref","first-page":"347","DOI":"10.1016\/j.conbuildmat.2019.03.184","article-title":"Effect of freeze-thaw cycles on mechanical and porosity properties of recycled construction waste mixtures","volume":"210","author":"Li","year":"2019","journal-title":"Constr. Build. Mater."},{"key":"ref_38","doi-asserted-by":"crossref","first-page":"1","DOI":"10.1016\/j.buildenv.2016.09.030","article-title":"Durability assessment of nanostructured TiO2 coatings applied on limestones to enhance building surface with self-cleaning ability","volume":"110","author":"Calia","year":"2016","journal-title":"Build. Environ."},{"key":"ref_39","doi-asserted-by":"crossref","unstructured":"Nogueira, R., Ferreira Pinto, A.P., and Gomes, A. (2020). Artificial ageing by salt crystallization: Test protocol and salt distribution patterns in lime-based rendering mortars. J. Cult. Herit.","DOI":"10.1016\/j.culher.2020.01.013"},{"key":"ref_40","unstructured":"Hunt, A., and Ewing, R. (2008). Percolation Theory for Flow in Porous Media, Springer. [2nd ed.]. Lect. Notes in Phys."},{"key":"ref_41","doi-asserted-by":"crossref","first-page":"101136","DOI":"10.1016\/j.jobe.2019.101136","article-title":"Tensile bond strength of lime-based mortars: The role of the microstructure on their performance assessed by a new non-standard test method","volume":"29","author":"Santos","year":"2020","journal-title":"J. Build. Eng."},{"key":"ref_42","doi-asserted-by":"crossref","unstructured":"Hall, C., and Hoff, W.D. (2012). Water Transport in Brick, Stone and Concrete, Spon Press, Taylor & Francis Group.","DOI":"10.1201\/b12840"},{"key":"ref_43","doi-asserted-by":"crossref","first-page":"69","DOI":"10.1016\/j.culher.2006.06.007","article-title":"Assessment of synthetic polymeric coatings for the protection andpreservation of stone monuments","volume":"8","author":"Tsakalofa","year":"2007","journal-title":"J. Cult. Herit."},{"key":"ref_44","first-page":"395","article-title":"Evaluation of the durability of hydrophobic treatments on concrete architectural heritage","volume":"20","author":"Lucquiaud","year":"2015","journal-title":"Restor. Build. Monum."},{"key":"ref_45","doi-asserted-by":"crossref","first-page":"519","DOI":"10.1016\/j.conbuildmat.2019.02.085","article-title":"Evaluation of the freeze-thaw durability of surface-treated airportpavement concrete under adverse conditions","volume":"206","author":"Guo","year":"2019","journal-title":"Constr. Build. Mater."},{"key":"ref_46","doi-asserted-by":"crossref","first-page":"107","DOI":"10.1016\/j.cemconcomp.2015.02.004","article-title":"The influence of water-repellent admixtures on the behaviour and the effectiveness of Portland limestone cement mortars","volume":"59","author":"Falchi","year":"2015","journal-title":"Cem. Concr. Comp."}],"container-title":["Coatings"],"original-title":[],"language":"en","link":[{"URL":"https:\/\/www.mdpi.com\/2079-6412\/10\/4\/363\/pdf","content-type":"unspecified","content-version":"vor","intended-application":"similarity-checking"}],"deposited":{"date-parts":[[2025,10,11]],"date-time":"2025-10-11T09:16:06Z","timestamp":1760174166000},"score":1,"resource":{"primary":{"URL":"https:\/\/www.mdpi.com\/2079-6412\/10\/4\/363"}},"subtitle":[],"short-title":[],"issued":{"date-parts":[[2020,4,7]]},"references-count":46,"journal-issue":{"issue":"4","published-online":{"date-parts":[[2020,4]]}},"alternative-id":["coatings10040363"],"URL":"https:\/\/doi.org\/10.3390\/coatings10040363","relation":{},"ISSN":["2079-6412"],"issn-type":[{"value":"2079-6412","type":"electronic"}],"subject":[],"published":{"date-parts":[[2020,4,7]]}}}