{"status":"ok","message-type":"work","message-version":"1.0.0","message":{"indexed":{"date-parts":[[2026,9,14]],"date-time":"2026-09-14T12:15:45Z","timestamp":1789388145830,"version":"build-2803163510"},"reference-count":72,"publisher":"Japanese Society for Dental Materials and Devices","issue":"3","content-domain":{"domain":[],"crossmark-restriction":false},"short-container-title":["Dent. Mater. J.","Dental Materials Journal"],"published-print":{"date-parts":[[2021,5,25]]},"DOI":"10.4012\/dmj.2020-223","type":"journal-article","created":{"date-parts":[[2021,1,14]],"date-time":"2021-01-14T22:10:53Z","timestamp":1610662253000},"page":"606-614","source":"Crossref","is-referenced-by-count":15,"title":["Fracture strength of endodontically treated premolars restored with different post systems and metal-ceramic or monolithic zirconia crowns"],"prefix":"10.4012","volume":"40","author":[{"given":"Anna","family":"MASTROGIANNI","sequence":"first","affiliation":[{"name":"Department of Prosthodontics, School of Dentistry, Aristotle University of Thessaloniki"}],"role":[{"vocabulary":"crossref","role":"author"}]},{"given":"Evdokia-Anna","family":"LIOLIOU","sequence":"additional","affiliation":[{"name":"Department of Prosthodontics, School of Dentistry, Aristotle University of Thessaloniki"}],"role":[{"vocabulary":"crossref","role":"author"}]},{"given":"Dimitrios","family":"TORTOPIDIS","sequence":"additional","affiliation":[{"name":"Department of Prosthodontics, School of Dentistry, Aristotle University of Thessaloniki"}],"role":[{"vocabulary":"crossref","role":"author"}]},{"given":"Christos","family":"GOGOS","sequence":"additional","affiliation":[{"name":"Department of Endodontology, School of Dentistry, Aristotle University of Thessaloniki"}],"role":[{"vocabulary":"crossref","role":"author"}]},{"given":"Eleana","family":"KONTONASAKI","sequence":"additional","affiliation":[{"name":"Department of Prosthodontics, School of Dentistry, Aristotle University of Thessaloniki"}],"role":[{"vocabulary":"crossref","role":"author"}]},{"given":"Petros","family":"KOIDIS","sequence":"additional","affiliation":[{"name":"Department of Prosthodontics, School of Dentistry, Aristotle University of Thessaloniki"}],"role":[{"vocabulary":"crossref","role":"author"}]}],"member":"2427","reference":[{"key":"1","unstructured":"1) Fernandes AS, Dessai GS. Factors affecting the fracture resistance of post-core reconstructed teeth: a review. Int J Prosthodont 2001; 14: 355-363."},{"key":"2","doi-asserted-by":"crossref","unstructured":"2) Evangelinaki E, Tortopidis D, Kontonasaki E, Fragou T, Gogos C, Koidis P. Effect of a crown ferrule on the fracture strength of endodontically treated canines restored with fiber posts and metal-ceramic or all-ceramic crowns. Int J Prosthodont 2013; 26: 384-387.","DOI":"10.11607\/ijp.3409"},{"key":"3","doi-asserted-by":"crossref","unstructured":"3) Pereira JR, De Ornelas F, Conti PC, Do Valle AL. Effect of a crown ferrule on the fracture resistance of endodontically treated teeth restored with prefabricated posts. J Prosthet Dent 2006; 95: 50-54.","DOI":"10.1016\/j.prosdent.2005.10.019"},{"key":"4","doi-asserted-by":"crossref","unstructured":"4) Sorensen JA, Martinoff JT. Intracoronal reinforcement and coronal coverage: A study of endodontically treated teeth. J Prosthet Dent 1984; 51: 780-784.","DOI":"10.1016\/0022-3913(84)90376-7"},{"key":"5","doi-asserted-by":"crossref","unstructured":"5) Aquilino SA, Caplan DJ. Relationship between crown placement and the survival of endodontically treated teeth. J Prosthet Dent 2002; 87: 256-263.","DOI":"10.1067\/mpr.2002.122014"},{"key":"6","doi-asserted-by":"crossref","unstructured":"6) Schwartz RS, Robbins JW. Post placement and restoration of endodontically treated teeth. J Endod 2004; 14: 289-301.","DOI":"10.1097\/00004770-200405000-00001"},{"key":"7","doi-asserted-by":"crossref","unstructured":"7) Akkayan B, G\u00fclmez T. Resistance to fracture of endodontically treated teeth restored with different post systems. J Prosthet Dent 2002; 87: 431-437.","DOI":"10.1067\/mpr.2002.123227"},{"key":"8","doi-asserted-by":"crossref","unstructured":"8) Figueiredo FED, Martins-Filho PRS, Faria-E-Silva AL. Do metal post-retained restorations result in more root fractures than fiber post-retained restorations? A systematic review and meta-analysis. J Endod 2015; 41: 309-316.","DOI":"10.1016\/j.joen.2014.10.006"},{"key":"9","doi-asserted-by":"crossref","unstructured":"9) Mangold JT, Kern M. Influence of glass-fiber posts on the fracture resistance and failure pattern of endodontically treated premolars with varying substance loss: An in vitro study. J Prosthet Dent 2011; 105: 387-393.","DOI":"10.1016\/S0022-3913(11)60080-2"},{"key":"10","doi-asserted-by":"crossref","unstructured":"10) Sherfudhin H, Hobeich J, Carvalho CA, Aboushelib MN, Sadig W, Salameh Z. Effect of different ferrule designs on the fracture resistance and failure pattern of endodontically treated teeth restored with fiber posts and all-ceramic crowns. J Appl Oral Sci 2011; 19: 28-33.","DOI":"10.1590\/S1678-77572011000100007"},{"key":"11","doi-asserted-by":"crossref","unstructured":"11) Samran A, Al-Afandi M, Kadour JA, Kern M. Effect of ferrule location on the fracture resistance of crowned mandibular premolars: An in vitro study. J Prosthet Dent 2015; 114: 86-91.","DOI":"10.1016\/j.prosdent.2014.12.014"},{"key":"12","doi-asserted-by":"crossref","unstructured":"12) Dua N, Kumar B, Arunagiri D, Iqbal M, Pushpa S, Hussain J. Comparative evaluation of the effect of different crown ferrule designs on the fracture resistance of endodontically treated mandibular premolars restored with fiber posts, composite cores, and crowns: An ex-vivo study. J Conserv Dent 2016; 19: 264.","DOI":"10.4103\/0972-0707.181945"},{"key":"13","doi-asserted-by":"crossref","unstructured":"13) Kar S, Tripathi A, Trivedi C. Effect of different ferrule length on fracture resistance of endodontically treated teeth: An in vitro study. J Clin Diagnostic Res 2017; 11: ZC49-52.","DOI":"10.7860\/JCDR\/2017\/24669.9675"},{"key":"14","doi-asserted-by":"crossref","unstructured":"14) Schmitter M, Rammelsberg P, Lenz J, Scheuber S, Schweizerhof K, Rues S. Teeth restored using fiber-reinforced posts: In vitro fracture tests and finite element analysis. Acta Biomater 2010; 6: 3747-3754.","DOI":"10.1016\/j.actbio.2010.03.012"},{"key":"15","doi-asserted-by":"crossref","unstructured":"15) Plotino G, Grande NM, Bedini R, Pameijer CH, Somma F. Flexural properties of endodontic posts and human root dentin. Dent Mater 2007; 23: 1129-1135.","DOI":"10.1016\/j.dental.2006.06.047"},{"key":"16","unstructured":"16) Creugers NHJ, Mentink AGM, Fokkinga WA, Kreulen CM. 5-year follow-up of a prospective clinical study on various types of core restorations. J Esthet Restor Dent 2012; 24: 74-76."},{"key":"17","doi-asserted-by":"crossref","unstructured":"17) Spazzin AO, Galafassi D, De Meira-J\u00fanior AD, Braz R, Garbin CA. Influence of post and resin cement on stress distribution of maxillary central incisors restored with direct resin composite. Oper Dent 2009; 34: 223-229.","DOI":"10.2341\/08-73"},{"key":"18","doi-asserted-by":"crossref","unstructured":"18) Mclaren JD, Mclaren CI, Yaman P, Bin-Shuwaish MS, Dennison JD, McDonald NJ. The effect of post type and length on the fracture resistance of endodontically treated teeth. J Prosthet Dent 2009; 101: 174-182.","DOI":"10.1016\/S0022-3913(09)60024-X"},{"key":"19","doi-asserted-by":"crossref","unstructured":"19) Zhou L, Wang Q. Comparison of fracture resistance between cast posts and fiber posts: a meta-analysis of literature. J Endod 2013; 39: 11-15.","DOI":"10.1016\/j.joen.2012.09.026"},{"key":"20","doi-asserted-by":"crossref","unstructured":"20) Al-Wahadni AM, Hamdan S, Al-Omiri M, Hammad MM, Hatamleh MM. Fracture resistance of teeth restored with different post systems: in vitro study. Oral Surg Oral Med Oral Pathol Oral Radiol Endod 2008; 106: e77-83.","DOI":"10.1016\/j.tripleo.2008.03.038"},{"key":"21","unstructured":"21) Bolhuis HPB, De Gee AJ, Feilzer AJ, Davidson CL. Fracture strength of different core build-up designs. Am J Dent 2001; 14: 286-290."},{"key":"22","doi-asserted-by":"crossref","unstructured":"22) Cormier CJ, Burns DR, Moon P. In vitro comparison of the fracture resistance and failure mode of fiber, ceramic, and conventional post systems at various stages of restoration. J Prosthodont 2001; 10: 26-36.","DOI":"10.1053\/jpro.2001.23777"},{"key":"23","unstructured":"23) Dietschi D, Duc O, Krejci I, Sadan A. Biomechanical considerations for the restoration of endodontically treated teeth: a systematic review of the literature-Part 1. Composition and micro- and macrostructure alterations. Quintessence Int 2007; 38: 733-743."},{"key":"24","doi-asserted-by":"crossref","unstructured":"24) King PA, Setchell DJ, Rees JS. Clinical evaluation of a carbon fibre reinforced carbon endodontic post. J Oral Rehabil 2003; 30: 785-789.","DOI":"10.1046\/j.1365-2842.2003.01178.x"},{"key":"25","doi-asserted-by":"crossref","unstructured":"25) Sarkis-Onofre R, Jacinto RDC, Boscato N, Cenci MS, Pereira-Cenci T. Cast metal vs. glass fibre posts: A randomized controlled trial with up to 3 years of follow up. J Dent 2014; 42: 582-587.","DOI":"10.1016\/j.jdent.2014.02.003"},{"key":"26","doi-asserted-by":"crossref","unstructured":"26) Sterzenbach G, Franke A, Naumann M. Rigid versus flexible dentine-like endodontic posts-Clinical testing of a biomechanical concept: Seven-year results of a randomized controlled clinical pilot trial on endodontically treated abutment teeth with severe hard tissue loss. J Endod 2012; 38: 1557-1563.","DOI":"10.1016\/j.joen.2012.08.015"},{"key":"27","doi-asserted-by":"crossref","unstructured":"27) Hayashi M, Takahashi Y, Imazato S, Ebisu S. Fracture resistance of pulpless teeth restored with post-cores and crowns. Dent Mater 2006; 22: 477-485.","DOI":"10.1016\/j.dental.2005.03.017"},{"key":"28","doi-asserted-by":"crossref","unstructured":"28) Salameh Z, Sorrentino R, Ounsi HF, Goracci C, Tashkandi E, Tay FR, <i>et al.<\/i> Effect of different all-ceramic crown system on fracture resistance and failure pattern of endodontically treated maxillary premolars restored with and without glass fiber posts. J Endod 2007; 33: 848-851.","DOI":"10.1016\/j.joen.2007.01.017"},{"key":"29","doi-asserted-by":"crossref","unstructured":"29) Fokkinga WA, Kreulen CM, Le Bell-R\u00f6nnl\u00f6f AM, Lassila LVJ, Vallittu PK, Creugers NH. In vitro fracture behavior of maxillary premolars with metal crowns and several post-and-core systems. Eur J Oral Sci 2006; 114: 250-256.","DOI":"10.1111\/j.1600-0722.2006.00357.x"},{"key":"30","unstructured":"30) Monticelli F, Grandini S, Goracci CFM. Clinical behavior of translucent fiber posts: A 2-year prospective study. Int J Prosthodont 2003; 16: 593-596"},{"key":"31","doi-asserted-by":"crossref","unstructured":"31) Freedman GA. Esthetic post-and-core treatment. Dent Clin North Am 2001; 45: 103-116.","DOI":"10.1016\/S0011-8532(22)00470-0"},{"key":"32","doi-asserted-by":"crossref","unstructured":"32) Sirimai S, Riis DN, Morgano SM. An in vitro study of the fracture resistance and the incidence of vertical root fracture of pulpless teeth restored with six post-and-core systems. J Prosthet Dent 1999; 81: 262-269.","DOI":"10.1016\/S0022-3913(99)70267-2"},{"key":"33","doi-asserted-by":"crossref","unstructured":"33) Torres-S\u00e1nchez C, Montoya-Salazar V, C\u00f3rdoba P, V\u00e9lez C, Guzm\u00e1n-Duran A, Gutierrez-P\u00e9rez JL, <i>et al.<\/i> Fracture resistance of endodontically treated teeth restored with glass fiber reinforced posts and cast gold post and cores cemented with three cements. J Prosthet Dent 2013; 110: 127-133.","DOI":"10.1016\/S0022-3913(13)60352-2"},{"key":"34","doi-asserted-by":"crossref","unstructured":"34) Abdelaziz KM, Khalil AA, Alsalhi IY, Almufarrij AJ, Mojathel AY. Fracture resistance of tilted premolars restored with different post-core systems. J Int Soc Prev Community Dent 2017; 7: 344-350.","DOI":"10.4103\/jispcd.JISPCD_382_17"},{"key":"35","doi-asserted-by":"crossref","unstructured":"35) Forberger N, G\u00f6hring TN. Influence of the type of post and core on in vitro marginal continuity, fracture resistance, and fracture mode of lithia disilicate-based all-ceramic crowns. J Prosthet Dent 2008 ;100: 264-273.","DOI":"10.1016\/S0022-3913(08)60205-X"},{"key":"36","doi-asserted-by":"crossref","unstructured":"36) Habibzadeh S, Rajati HR, Hajmiragha H, Esmailzadeh S, Kharazifard M. Fracture resistances of zirconia, cast Ni-Cr, and fiber-glass composite posts under all-ceramic crowns in endodontically treated premolars. J Adv Prosthodont 2017; 9: 170-175.","DOI":"10.4047\/jap.2017.9.3.170"},{"key":"37","doi-asserted-by":"crossref","unstructured":"37) Gu XH, Kern M. Fracture resistance of crowned incisors with different post systems and luting agents. J Oral Rehabil 2006; 33: 918-923.","DOI":"10.1111\/j.1365-2842.2006.01672.x"},{"key":"38","doi-asserted-by":"crossref","unstructured":"38) Ploumaki A, Bilkhair A, Tuna T, Stampf S, Strub JR. Success rates of prosthetic restorations on endodontically treated teeth; a systematic review after 6 years. J Oral Rehabil 2013; 40: 618-630.","DOI":"10.1111\/joor.12058"},{"key":"39","doi-asserted-by":"crossref","unstructured":"39) Varvara G, Perinetti G, Di Iorio D, Murmura G, Caputi S. In vitro evaluation of fracture resistance and failure mode of internally restored endodontically treated maxillary incisors with differing heights of residual dentin. J Prosthet Dent 2007; 98: 365-372.","DOI":"10.1016\/S0022-3913(07)60121-8"},{"key":"40","unstructured":"40) Butz F, Lennon AM, Heydecke G, Strub JR. Survival rate and fracture strength of endodontically treated maxillary incisors with moderate defects restored with different post-and-core systems: an in vitro study. Int J Prosthodont 2001; 14: 58-64."},{"key":"41","unstructured":"41) Schmitter MRP. Survival of two post systems: Five-year results of a randomized clinical trial. Quintessence Int 2011; 42: 843-850."},{"key":"42","doi-asserted-by":"crossref","unstructured":"42) Cloet E, Debels E, Naert I. Controlled clinical trial on the outcome of glass fiber composite cores versus wrought posts and cast cores for the restoration of endodontically treated teeth: A 5-year follow-up study. Int J Prosthodont 2017; 30: 71-79.","DOI":"10.11607\/ijp.4861"},{"key":"43","doi-asserted-by":"crossref","unstructured":"43) Shahrbaf S, Mirzakouchaki B, Oskoui SS, Kahnamoui MA. The effect of marginal ridge thickness on the fracture resistance of endodontically-treated, composite restored maxillary premolars. Oper Dent 2007; 32: 285-290.","DOI":"10.2341\/06-83"},{"key":"44","doi-asserted-by":"crossref","unstructured":"44) Aur\u00e9lio IL, Fraga S, Rippe MP, Valandro LF. Are posts necessary for the restoration of root filled teeth with limited tissue loss? A structured review of laboratory and clinical studies. Int Endod J 2016; 49: 827-835.","DOI":"10.1111\/iej.12538"},{"key":"45","doi-asserted-by":"crossref","unstructured":"45) Stavropoulou AF, Koidis PT. A systematic review of single crowns on endodontically treated teeth. J Dent 2007; 35: 761-767.","DOI":"10.1016\/j.jdent.2007.07.004"},{"key":"46","doi-asserted-by":"crossref","unstructured":"46) Attia A, Abdelaziz KM, Freitag S, Kern M. Fracture load of composite resin and feldspathic all-ceramic CAD\/CAM crowns. J Prosthet Dent 2006; 95: 117-123.","DOI":"10.1016\/j.prosdent.2005.11.014"},{"key":"47","doi-asserted-by":"crossref","unstructured":"47) Helkimo E, Carlsson GE, Helkimo M. Bite force and state of dentition. Acta Odontol Scand 1977; 35: 297-303.","DOI":"10.3109\/00016357709064128"},{"key":"48","doi-asserted-by":"crossref","unstructured":"48) Tortopidis D, Lyons MF, Baxendale RH, Gilmour WH. The variability of bite force measurement between sessions, in different positions within the dental arch. J Oral Rehabil 1998; 25: 681-686.","DOI":"10.1046\/j.1365-2842.1998.00293.x"},{"key":"49","unstructured":"49) Yoshinari MDT. Fracture strength of all-ceramic crowns. Int J Prosthodont 1994; 7: 329-338."},{"key":"50","doi-asserted-by":"crossref","unstructured":"50) Gibbs CH, Mahan PE, Mauderli A, Lundeen HC, Walsh EK. Limits of human bite strength. J Prosthet Dent 1986; 56: 226-229.","DOI":"10.1016\/0022-3913(86)90480-4"},{"key":"51","doi-asserted-by":"crossref","unstructured":"51) Ingervall B, Helkimo E. Masticatory muscle force and facial morphology in man. Arch Oral Biol 1978; 23: 203-206.","DOI":"10.1016\/0003-9969(78)90217-0"},{"key":"52","doi-asserted-by":"crossref","unstructured":"52) Lyons MF, Baxendale RH. A preliminary electromyographic study of bite force and jaw-closing muscle fatigue in human subjects with advanced tooth wear. J Oral Rehabil 1990; 17: 311-318.","DOI":"10.1111\/j.1365-2842.1990.tb00014.x"},{"key":"53","doi-asserted-by":"crossref","unstructured":"53) Johansson A, Omar R, Carlsson GE. Bruxism and prosthetic treatment: A critical review. J Prosthodont Res 2011; 55: 127-136.","DOI":"10.1016\/j.jpor.2011.02.004"},{"key":"54","doi-asserted-by":"crossref","unstructured":"54) Hamza TA, Sherif RM. Fracture resistance of monolithic glass-ceramics versus bilayered zirconia-based restorations. J Prosthodont 2017; 28: e259-e264.","DOI":"10.1111\/jopr.12684"},{"key":"55","doi-asserted-by":"crossref","unstructured":"55) Schriwer C, Skjold A, Gjerdet Nr, \u00d8ilo M. Monolithic zirconia dental crowns. Internal fit, margin quality, fracture mode and load at fracture. Dent Mater 2017; 33: 1012-1020.","DOI":"10.1016\/j.dental.2017.06.009"},{"key":"56","doi-asserted-by":"crossref","unstructured":"56) Kontonasaki E, Giasimakopoulos P, Rigos AE. Strength and aging resistance of monolithic zirconia: an update to current knowledge. Jpn Dent Sci Rev 2020; 56: 1-23.","DOI":"10.1016\/j.jdsr.2019.09.002"},{"key":"57","doi-asserted-by":"crossref","unstructured":"57) Kontonasaki E, Rigos AE, Ilia C, Istantsos T. Monolithic zirconia: An update to current knowledge. Optical properties, wear, and clinical performance. Dent J 2019; 7: 1-23.","DOI":"10.3390\/dj7030090"},{"key":"58","doi-asserted-by":"crossref","unstructured":"58) Kapagiannidis D, Kontonasaki E, Bikos P, Koidis P. Teeth and gingival display in the premolar area during smiling in relation to gender and age. J Oral Rehabil 2005; 32: 830-837.","DOI":"10.1111\/j.1365-2842.2005.01517.x"},{"key":"59","doi-asserted-by":"crossref","unstructured":"59) Peck CC. Biomechanics of occlusion: implications for oral rehabilitation. J Oral Rehabil 2016; 43: 205-214.","DOI":"10.1111\/joor.12345"},{"key":"60","doi-asserted-by":"crossref","unstructured":"60) Lin J, Matinlinna JP, Shinya A, Botelho MG, Zheng Z. Effect of fiber post length and abutment height on fracture resistance of endodontically treated premolars prepared for zirconia crowns. Odontology 2018; 106: 215-222.","DOI":"10.1007\/s10266-017-0320-7"},{"key":"61","doi-asserted-by":"crossref","unstructured":"61) Zeola LF, Pereira FA, Machado AC, Reis BR, Kaidonis J, Xie Z, <i>et al.<\/i> Effects of non-carious cervical lesion size, occlusal loading and restoration on biomechanical behaviour of premolar teeth. Aust Dent J 2016; 61: 408-417.","DOI":"10.1111\/adj.12391"},{"key":"62","doi-asserted-by":"crossref","unstructured":"62) Eskita\u015fcio\u01e7lu G, Belli S, Kalkan M. Evaluation of two post core systems using two different methods (fracture strength test and a finite elemental stress analysis). J Endod 2002; 28: 629-633.","DOI":"10.1097\/00004770-200209000-00001"},{"key":"63","doi-asserted-by":"crossref","unstructured":"63) Pegoretti A, Fambri L, Zappini G, Bianchetti M. Finite element analysis of a glass fibre reinforced composite endodontic post. Biomaterials 2002; 23: 2667-2682.","DOI":"10.1016\/S0142-9612(01)00407-0"},{"key":"64","doi-asserted-by":"crossref","unstructured":"64) Nakabayashi N, Watanabe AGN. Dentin adhesion of \u201cmodified\u201d 4-META\/MMA-TBB resin: function of HEMA. Dent Mater 1992; 8: 259-264.","DOI":"10.1016\/0109-5641(92)90096-U"},{"key":"65","doi-asserted-by":"crossref","unstructured":"65) Titley KC, Chernecky R, Rossouw PE, Kulkarni GV. The effect of various storage methods and media on shear-bond strengths of dental composite resin to bovine dentine. Arch Oral Biol 1998; 43: 305-311.","DOI":"10.1016\/S0003-9969(97)00112-X"},{"key":"66","doi-asserted-by":"crossref","unstructured":"66) Delong R, Douglas WH. Development of an artificial oral environment for the testing of dental restoratives: bi-axial force and movement control. J Dent Res 1983; 62: 32-36.","DOI":"10.1177\/00220345830620010801"},{"key":"67","doi-asserted-by":"crossref","unstructured":"67) Naumann M, Metzdorf G, Fokkinga W, Watzke R, Sterzenbach G, Bayne S, <i>et al.<\/i> Influence of test parameters on in vitro fracture strength of post-endodontic restorations: A structured review. J Oral Rehabil 2009; 36: 299-312.","DOI":"10.1111\/j.1365-2842.2009.01940.x"},{"key":"68","doi-asserted-by":"crossref","unstructured":"68) Miura S, Kasahara S, Yamauchi S, Egusa H. Effect of finish line design on stress distribution in bilayer and monolithic zirconia crowns: a three-dimensional finite element analysis study. Eur J Oral Sci 2018; 126: 159-165.","DOI":"10.1111\/eos.12402"},{"key":"69","unstructured":"69) Mehta C, Patel R. (1996). SPSS Exact Tests 7.0 for Windows. Chicago: SPSS Inc."},{"key":"70","doi-asserted-by":"crossref","unstructured":"70) \u00d8ilo M, Hardang AD, Ulsund AH, Gjerdet NR. Fractographic features of glass-ceramic and zirconia-based dental restorations fractured during clinical function. Eur J Oral Sci 2014; 122: 238-244.","DOI":"10.1111\/eos.12127"},{"key":"71","doi-asserted-by":"crossref","unstructured":"71) Meira JBC, Esp\u00f3sito COM, Quitero MFZ, Poiate IAVP, Pfeifer CSC, Tanaka CB, <i>et al<\/i>. Elastic modulus of posts and the risk of root fracture. Dent Traumatol 2009; 25: 394-398.","DOI":"10.1111\/j.1600-9657.2009.00772.x"},{"key":"72","doi-asserted-by":"crossref","unstructured":"72) Camposilvan E, Leone R, Gremillard L, Sorrentino R, Zarone F, Ferrari M, <i>et al<\/i>. Aging resistance, mechanical properties and translucency of different yttria-stabilized zirconia ceramics for monolithic dental crown applications. Dent Mater 2018; 34: 879-890.","DOI":"10.1016\/j.dental.2018.03.006"}],"container-title":["Dental Materials Journal"],"original-title":[],"language":"en","link":[{"URL":"https:\/\/www.jstage.jst.go.jp\/article\/dmj\/40\/3\/40_2020-223\/_pdf","content-type":"unspecified","content-version":"vor","intended-application":"similarity-checking"}],"deposited":{"date-parts":[[2022,12,11]],"date-time":"2022-12-11T16:52:17Z","timestamp":1670777537000},"score":1,"resource":{"primary":{"URL":"https:\/\/www.jstage.jst.go.jp\/article\/dmj\/40\/3\/40_2020-223\/_article"}},"subtitle":[],"short-title":[],"issued":{"date-parts":[[2021,5,25]]},"references-count":72,"journal-issue":{"issue":"3","published-print":{"date-parts":[[2021]]}},"URL":"https:\/\/doi.org\/10.4012\/dmj.2020-223","relation":{},"ISSN":["0287-4547","1881-1361"],"issn-type":[{"value":"0287-4547","type":"print"},{"value":"1881-1361","type":"electronic"}],"subject":[],"published":{"date-parts":[[2021,5,25]]}}}