{"status":"ok","message-type":"work","message-version":"1.0.0","message":{"indexed":{"date-parts":[[2026,5,13]],"date-time":"2026-05-13T10:58:56Z","timestamp":1778669936395,"version":"3.51.4"},"reference-count":33,"publisher":"Japanese Society for Dental Materials and Devices","issue":"2","content-domain":{"domain":[],"crossmark-restriction":false},"short-container-title":["Dent. Mater. J.","Dental Materials Journal"],"published-print":{"date-parts":[[2022,3,25]]},"DOI":"10.4012\/dmj.2021-090","type":"journal-article","created":{"date-parts":[[2021,12,3]],"date-time":"2021-12-03T22:09:37Z","timestamp":1638569377000},"page":"249-255","source":"Crossref","is-referenced-by-count":8,"title":["Effect of supporting dies\u2019 mechanical properties on fracture behavior of monolithic zirconia molar crowns"],"prefix":"10.4012","volume":"41","author":[{"given":"Yutao","family":"JIAN","sequence":"first","affiliation":[{"name":"Institute of Stomatological Research, Guangdong Provincial Key Laboratory of Stomatology, Sun Yat-Sen University"}],"role":[{"role":"author","vocabulary":"crossref"}]},{"given":"Tianyi","family":"ZHANG","sequence":"additional","affiliation":[{"name":"Research Center for Stomatology, Peking University Shenzhen Hospital"}],"role":[{"role":"author","vocabulary":"crossref"}]},{"given":"Xiaodong","family":"WANG","sequence":"additional","affiliation":[{"name":"Department of Prosthodontics, Guanghua School of Stomatology, Sun Yat-Sen University; Guangdong Engineering Research Center of Technology and Materials for Oral Reconstruction, Guangdong Provincial Key Laboratory of Stomatology"}],"role":[{"role":"author","vocabulary":"crossref"}]},{"given":"Laina","family":"KYAW","sequence":"additional","affiliation":[{"name":"Department of Prosthodontics, Guanghua School of Stomatology, Sun Yat-Sen University; Guangdong Engineering Research Center of Technology and Materials for Oral Reconstruction, Guangdong Provincial Key Laboratory of Stomatology"}],"role":[{"role":"author","vocabulary":"crossref"}]},{"given":"Edmond Ho Nang","family":"POW","sequence":"additional","affiliation":[{"name":"Prosthodontics, Faculty of Dentistry, The University of Hong Kong, Prince Philip Dental Hospital"}],"role":[{"role":"author","vocabulary":"crossref"}]},{"given":"Ke","family":"ZHAO","sequence":"additional","affiliation":[{"name":"Department of Prosthodontics, Guanghua School of Stomatology, Sun Yat-Sen University; Guangdong Engineering Research Center of Technology and Materials for Oral Reconstruction, Guangdong Provincial Key Laboratory of Stomatology"}],"role":[{"role":"author","vocabulary":"crossref"}]}],"member":"2427","reference":[{"key":"1","doi-asserted-by":"crossref","unstructured":"1) Rekow ED, Silva NRFA, Coelho PG, Zhang Y, Guess P, Thompson VP. Performance of dental ceramics: challenges for improvements. J Dent Res 2011; 90: 937-952.","DOI":"10.1177\/0022034510391795"},{"key":"2","unstructured":"2) Lee SK, Wilson PR. Fracture strength of all-ceramic crowns with varying core elastic moduli. Aust Dent J 2000; 45: 103-107."},{"key":"3","unstructured":"3) Rosentritt M, Reill M, Naumann M, Nowak A, Handel G. Strength investigation of artificial substitutes for human teeth in in vitro studies. Int J Prosthodont 2009; 22: 62-64."},{"key":"4","doi-asserted-by":"crossref","unstructured":"4) Rosentritt M, Naumann M, Hahnel S, Handel G, Reill M. Evaluation of tooth analogs and type of restoration on the fracture resistance of post and core restored incisors. J Biomed Mater Res B Appl Biomater 2009; 91: 272-276.","DOI":"10.1002\/jbm.b.31399"},{"key":"5","doi-asserted-by":"crossref","unstructured":"5) Joda T, Huber S, B\u00fcrki A, Zysset P, Br\u00e4gger U. Influence of abutment design on stiffness, strength, and failure of implant-supported monolithic resin nano ceramic (RNC) crowns. Clin Implant Dent Relat Res 2015; 17: 1200-1207.","DOI":"10.1111\/cid.12215"},{"key":"6","doi-asserted-by":"crossref","unstructured":"6) Lameira DP, Buarque e Silva WA, Andrade e Silva F, De Souza GM. Fracture strength of aged monolithic and bilayer zirconia-based crowns. Biomed Res Int 2015; 2015: 418641.","DOI":"10.1155\/2015\/418641"},{"key":"7","doi-asserted-by":"crossref","unstructured":"7) Johansson C, Kmet G, Rivera J, Larsson C, Vult Von Steyern P. Vult Von Steyern P. Fracture strength of monolithic all-ceramic crowns made of high translucent yttrium oxide-stabilized zirconium dioxide compared to porcelain-veneered crowns and lithium disilicate crowns. Acta Odontol Scand 2014; 72: 145-153.","DOI":"10.3109\/00016357.2013.822098"},{"key":"8","doi-asserted-by":"crossref","unstructured":"8) Beuer F, Stimmelmayr M, Gueth JF, Edelhoff D, Naumann M.In vitro performance of full-contour zirconia single crowns. Dent Mater 2012; 28: 449-456.","DOI":"10.1016\/j.dental.2011.11.024"},{"key":"9","doi-asserted-by":"crossref","unstructured":"9) Sorrentino R, Triulzio C, Tricarico MG, Bonadeo G, Gherlone EF, Ferrari M. In vitro analysis of the fracture resistance of CAD-CAM monolithic zirconia molar crowns with different occlusal thickness. J Mech Behav Biomed Mater 2012; 61: 328-333.","DOI":"10.1016\/j.jmbbm.2016.04.014"},{"key":"10","doi-asserted-by":"crossref","unstructured":"10) Yucel MT, Yondem I, Aykent F, Eraslan O. Influence of the supporting die structures on the fracture strength of all-ceramic materials. Clin Oral Investig 2012; 16: 1105-1110.","DOI":"10.1007\/s00784-011-0606-z"},{"key":"11","doi-asserted-by":"crossref","unstructured":"11) Oilo M, Kvam K, Gjerdet NR. Simulation of clinical fractures for three different all-ceramic crowns. Eur J Oral Sci 2014; 122: 245-250.","DOI":"10.1111\/eos.12128"},{"key":"12","doi-asserted-by":"crossref","unstructured":"12) Nakamura K, Mouhat M, Nerg\u00e5rd JM, L\u00e6greid SJ, Kanno T, Milleding P, <i>et al<\/i>. Effect of cements on fracture resistance of monolithic zirconia crowns. Acta Biomater Odontol Scand 2016; 2: 12-19.","DOI":"10.3109\/23337931.2015.1129908"},{"key":"13","doi-asserted-by":"crossref","unstructured":"13) Zhang Y, Mai Z, Barani A, Bush M, Lawn B. Fracture-resistant monolithic dental crowns. Dent Mater 2016; 32: 442-449.","DOI":"10.1016\/j.dental.2015.12.010"},{"key":"14","doi-asserted-by":"crossref","unstructured":"14) Pallis K, Griggs JA, Woody RD, Guillen GE, Miller AW. Fracture resistance of three all-ceramic restorative systems for posterior applications. J Prosthet Dent 2004; 91: 561-569.","DOI":"10.1016\/j.prosdent.2004.03.001"},{"key":"15","doi-asserted-by":"crossref","unstructured":"15) Jian YT, Yang Y, Tian T, Stanford C, Zhang XP, Zhao K. Correction: Effect of pore size and porosity on the biomechanical properties and cytocompatibility of porous NiTi alloys. PloS One 2015; 10: e0128138.","DOI":"10.1371\/journal.pone.0128138"},{"key":"16","unstructured":"16) ASTM, E111-04. 2010. Standard test method for Young\u2019s modulus, tangent modulus, and chord modulus. West Conshohocken, PA, USA, 2010."},{"key":"17","unstructured":"17) ASTM, E399. 2012. Standard test method for linear-elastic plane-strain fracture toughness KIC of metallic materials. West Conshohocken, PA, USA, 2012."},{"key":"18","unstructured":"18) ISO, 4049. 2000. Polymer based filling, restorative and luting materials International Organization for Standardization. 3rd ed. Url: https:\/\/www.iso.org\/standard\/23041.html"},{"key":"19","unstructured":"19) ISO 6507-1:2018. Metallic materials, Vickers hardness test. 4th ed. Url: https:\/\/www.iso.org\/standard\/64065.html"},{"key":"20","doi-asserted-by":"crossref","unstructured":"20) Jian Y, Dao L, Wang X, Zhang X, Swain MV, Zhao K. Influence of veneer pore defects on fracture behavior of bilayered lithium disilicate glass-ceramic crowns. Dent Mater 2019; 35: e83-e95.","DOI":"10.1016\/j.dental.2019.01.016"},{"key":"21","doi-asserted-by":"crossref","unstructured":"21) Sun T, Zhou S, Lai R, Liu R, Ma S, Zhou Z, <i>et al.<\/i> Load-bearing capacity and the recommended thickness of dental monolithic zirconia single crowns. J Mech Behav Biomed Mater 2014; 35: 93-101.","DOI":"10.1016\/j.jmbbm.2014.03.014"},{"key":"22","doi-asserted-by":"crossref","unstructured":"22) Bindl A, L\u00fcthy H, M\u00f6rmann WH. Strength and fracture pattern of monolithic CAD\/CAM-generated posterior crowns. Dent Mater 2006; 22: 29-36.","DOI":"10.1016\/j.dental.2005.02.007"},{"key":"23","doi-asserted-by":"crossref","unstructured":"23) Yamaguchi S, Katsumoto Y, Hayashi K, Aoki M, Kunikata M, Nakase Y, <i>et al.<\/i> Fracture origin and crack propagation of CAD\/CAM composite crowns by combining of in vitro and in silico approaches. J Mech Behav Biomed Mater 2020; 112: 104083.","DOI":"10.1016\/j.jmbbm.2020.104083"},{"key":"24","doi-asserted-by":"crossref","unstructured":"24) Wang XH, Li JS, Hu R, Kou HC. Mechanical properties and pore structure deformation behaviour of biomedical porous titanium. Transactions Nonferr Metal Soc 2015; 25: 1543-1550.","DOI":"10.1016\/S1003-6326(15)63756-6"},{"key":"25","doi-asserted-by":"crossref","unstructured":"25) Chaves FO, Farias NC, Medeiros LM, Alonso RC, Di Hip\u00f3lito V, D\u2019Alpino PH. Mechanical properties of composites as functions of the syringe storage temperature and energy dose. J Appl Oral Sci 2015; 23: 120-128.","DOI":"10.1590\/1678-775720130643"},{"key":"26","unstructured":"26) Rosentritt M, Plein T, Kolbeck C, Behr M, Handel G. In vitro fracture force and marginal adaptation of ceramic crowns fixed on natural and artificial teeth. Int J Prosthodont 1999; 13: 387-391."},{"key":"27","doi-asserted-by":"crossref","unstructured":"27) Chan YL, Ngan AH, King NM. Nano-scale structure and mechanical properties of the human dentine-enamel junction. J Mech Behav Biomed Mater 2011; 4: 785-795.","DOI":"10.1016\/j.jmbbm.2010.09.003"},{"key":"28","doi-asserted-by":"crossref","unstructured":"28) Zhang Y, Lee JJ, Srikanth R, Lawn BR. Edge chipping and flexural resistance of monolithic ceramics. Dent Mater 2013; 29: 1201-1208.","DOI":"10.1016\/j.dental.2013.09.004"},{"key":"29","doi-asserted-by":"crossref","unstructured":"29) de Kok P, Kleverlaan CJ, de Jager N, Kuijs R, Feilzer AJ. Mechanical performance of implant-supported posterior crowns. J Prosthet Dent 2015; 114: 59-66.","DOI":"10.1016\/j.prosdent.2014.10.015"},{"key":"30","doi-asserted-by":"crossref","unstructured":"30) Barani A, Chai H, Lawn BR, Bush MB. Mechanics analysis of molar tooth splitting. Acta Biomater 2015; 15: 237-243.","DOI":"10.1016\/j.actbio.2015.01.004"},{"key":"31","doi-asserted-by":"crossref","unstructured":"31) \u00d8ilo M, Gjerdet NR. Fractographic analyses of all-ceramic crowns: a study of 27 clinically fractured crowns. Dent Mater 2013; 29: e78-e84.","DOI":"10.1016\/j.dental.2013.03.018"},{"key":"32","doi-asserted-by":"crossref","unstructured":"32) Papadogiannis DY, Lakes RS, Papadogiannis Y, Palaghias G, Helvatjoglu-Antoniades M. The effect of temperature on the viscoelastic properties of nano-hybrid composites. Dent Mater 2008; 24: 257-266.","DOI":"10.1016\/j.dental.2007.05.009"},{"key":"33","doi-asserted-by":"crossref","unstructured":"33) Zesewitz TF, Knauber AW, Nothdurft FP. Fracture resistance of a selection of full-contour all-ceramic crowns: an in vitro study. Int J Prosthodont 2014; 27: 264-266.","DOI":"10.11607\/ijp.3815"}],"container-title":["Dental Materials Journal"],"original-title":[],"language":"en","link":[{"URL":"https:\/\/www.jstage.jst.go.jp\/article\/dmj\/41\/2\/41_2021-090\/_pdf","content-type":"unspecified","content-version":"vor","intended-application":"similarity-checking"}],"deposited":{"date-parts":[[2022,4,2]],"date-time":"2022-04-02T05:50:41Z","timestamp":1648878641000},"score":1,"resource":{"primary":{"URL":"https:\/\/www.jstage.jst.go.jp\/article\/dmj\/41\/2\/41_2021-090\/_article"}},"subtitle":[],"short-title":[],"issued":{"date-parts":[[2022,3,25]]},"references-count":33,"journal-issue":{"issue":"2","published-print":{"date-parts":[[2022]]}},"URL":"https:\/\/doi.org\/10.4012\/dmj.2021-090","relation":{},"ISSN":["0287-4547","1881-1361"],"issn-type":[{"value":"0287-4547","type":"print"},{"value":"1881-1361","type":"electronic"}],"subject":[],"published":{"date-parts":[[2022,3,25]]},"article-number":"2021-090"}}