{"status":"ok","message-type":"work","message-version":"1.0.0","message":{"indexed":{"date-parts":[[2026,7,9]],"date-time":"2026-07-09T22:50:57Z","timestamp":1783637457543,"version":"3.55.0"},"reference-count":34,"publisher":"Association for Materials Protection and Performance (AMPP)","issue":"10","content-domain":{"domain":[],"crossmark-restriction":false},"short-container-title":[],"published-print":{"date-parts":[[2014,10,1]]},"abstract":"<jats:p>Corrosion performance of austenitic-ferritic (duplex) stainless steels UNS S32101, S32202, S32304, and S32205 and austenitic stainless steels UNS S30403 and S31603 was studied in the presence of chloride deposits simulating non-rinsing atmospheric conditions. The effect of temperature, relative humidity, concentration, and composition of the chloride deposits on the tendency for atmospheric, low-temperature, chloride-induced stress corrosion cracking (SCC), pitting, and selective corrosion was assessed using prestressed samples with a circular weld. In the presence of calcium chloride, SCC was observed at temperatures as low as 20\u00b0C and 30\u00b0C on the austenitic stainless steels UNS S30403 (Type 304L) and UNS S31603 (Type 316L), respectively. The only cases of SCC of tested duplex stainless steel grades were found at 70\u00b0C, which otherwise suffered mainly selective dissolution of the ferrite phase with one order lower depth of attack. The initiation of SCC and selective\/pitting corrosion was governed by the equilibrium chloride concentration in a solution formed by contact with chloride-containing deposits and with air at a given relative humidity. Threshold levels of critical chloride concentrations, critical relative humidity in the presence of specific deposits, and maximum temperatures for safe applications of the studied grades were established.<\/jats:p>","DOI":"10.5006\/1242","type":"journal-article","created":{"date-parts":[[2014,6,16]],"date-time":"2014-06-16T19:04:49Z","timestamp":1402945489000},"page":"1052-1063","source":"Crossref","is-referenced-by-count":63,"title":["Low-Temperature Stress Corrosion Cracking of Austenitic and Duplex Stainless Steels Under Chloride Deposits"],"prefix":"10.5006","volume":"70","author":[{"given":"Tomas","family":"Prosek","sequence":"first","affiliation":[],"role":[{"vocabulary":"crossref","role":"author"}]},{"given":"Anne","family":"Le Gac","sequence":"additional","affiliation":[],"role":[{"vocabulary":"crossref","role":"author"}]},{"given":"Dominique","family":"Thierry","sequence":"additional","affiliation":[],"role":[{"vocabulary":"crossref","role":"author"}]},{"given":"Sandra","family":"Le Manchet","sequence":"additional","affiliation":[],"role":[{"vocabulary":"crossref","role":"author"}]},{"given":"Christian","family":"Lojewski","sequence":"additional","affiliation":[],"role":[{"vocabulary":"crossref","role":"author"}]},{"given":"Amelie","family":"Fanica","sequence":"additional","affiliation":[],"role":[{"vocabulary":"crossref","role":"author"}]},{"given":"Elisabeth","family":"Johansson","sequence":"additional","affiliation":[],"role":[{"vocabulary":"crossref","role":"author"}]},{"given":"Carolina","family":"Canderyd","sequence":"additional","affiliation":[],"role":[{"vocabulary":"crossref","role":"author"}]},{"given":"Francois","family":"Dupoiron","sequence":"additional","affiliation":[],"role":[{"vocabulary":"crossref","role":"author"}]},{"given":"Tom","family":"Snauwaert","sequence":"additional","affiliation":[],"role":[{"vocabulary":"crossref","role":"author"}]},{"given":"Fleur","family":"Maas","sequence":"additional","affiliation":[],"role":[{"vocabulary":"crossref","role":"author"}]},{"given":"Benny","family":"Droesbeke","sequence":"additional","affiliation":[],"role":[{"vocabulary":"crossref","role":"author"}]}],"member":"2917","published-online":{"date-parts":[[2014,6,16]]},"reference":[{"issue":"5","key":"2025031810193074200_i0010-9312-70-10-1052-b1","doi-asserted-by":"crossref","first-page":"331","DOI":"10.1002\/maco.200390073","volume":"54","author":"Faller","year":"2003","journal-title":"Mater. Corros"},{"key":"2025031810193074200_i0010-9312-70-10-1052-b2","article-title":"\u201cThe Stress Corrosion Cracking Behavior of Stainless Steel at Temperatures Below 50\u00b0C,\u201d","author":"Fielder","year":"1998"},{"issue":"6","key":"2025031810193074200_i0010-9312-70-10-1052-b3","first-page":"141","volume":"110","author":"N\u00fcrnberger","year":"1990","journal-title":"Stahl und Eisen"},{"key":"2025031810193074200_i0010-9312-70-10-1052-b4","doi-asserted-by":"crossref","first-page":"467","DOI":"10.1002\/maco.19890400803","volume":"40","author":"Herbsleb","year":"1989","journal-title":"Mater. Corros"},{"key":"2025031810193074200_i0010-9312-70-10-1052-b5","first-page":"762","article-title":"\u201cThe Corrosion of Stainless Steels in Swimming Pools,\u201d","volume":"vol. 2","author":"Fielder","year":"1992"},{"issue":"3","key":"2025031810193074200_i0010-9312-70-10-1052-b6","doi-asserted-by":"crossref","first-page":"173","DOI":"10.1179\/000705991798269233","volume":"26","author":"Oldfield","year":"1991","journal-title":"Br. Corros. J"},{"key":"2025031810193074200_i0010-9312-70-10-1052-b7","first-page":"21","article-title":"\u201cStress Corrosion Cracking of Stainless Steels in Swimming Pools,\u201d","author":"Heselmans","year":"2001"},{"issue":"9","key":"2025031810193074200_i0010-9312-70-10-1052-b8","volume":"82","author":"Baddoo","year":"2004","journal-title":"The Structural Engineer"},{"issue":"12","key":"2025031810193074200_i0010-9312-70-10-1052-b9","first-page":"66","volume":"29","author":"Dillon","year":"1990","journal-title":"Mater. Perform"},{"issue":"24","key":"2025031810193074200_i0010-9312-70-10-1052-b10","first-page":"416","volume":"66","author":"Page","year":"1988","journal-title":"The Structural Engineer"},{"issue":"5","key":"2025031810193074200_i0010-9312-70-10-1052-b11","doi-asserted-by":"crossref","first-page":"410","DOI":"10.1007\/s11668-008-9158-1","volume":"8","author":"Sjong","year":"2008","journal-title":"J. Fail. Anal. Prev"},{"key":"2025031810193074200_i0010-9312-70-10-1052-b12","doi-asserted-by":"crossref","first-page":"123","DOI":"10.1016\/j.engfailanal.2011.09.011","volume":"19","author":"Karalis","year":"2012","journal-title":"Eng. Fail. Anal"},{"issue":"12","key":"2025031810193074200_i0010-9312-70-10-1052-b13","first-page":"63","volume":"29","author":"Gnanamoorthy","year":"1990","journal-title":"Mater. Perform"},{"issue":"12","key":"2025031810193074200_i0010-9312-70-10-1052-b14","first-page":"60","volume":"29","author":"Kain","year":"1990","journal-title":"Mater. Perform"},{"key":"2025031810193074200_i0010-9312-70-10-1052-b15","first-page":"92","volume":"38","author":"Shoji","year":"1989","journal-title":"Boshoku Gijutsu"},{"issue":"10","key":"2025031810193074200_i0010-9312-70-10-1052-b16","doi-asserted-by":"crossref","first-page":"679","DOI":"10.1002\/maco.19970481004","volume":"48","author":"Arnold","year":"1997","journal-title":"Mater. Corros"},{"issue":"7","key":"2025031810193074200_i0010-9312-70-10-1052-b17","doi-asserted-by":"crossref","first-page":"482","DOI":"10.1002\/(SICI)1521-4176(199807)49:7<482::AID-MACO482>3.0.CO;2-M","volume":"49","author":"Arnold","year":"1998","journal-title":"Mater. Corros"},{"key":"2025031810193074200_i0010-9312-70-10-1052-b18","first-page":"99","article-title":"\u201cCorrosion Behaviour of Stainless Steels in the Atmosphere of Indoor Swimming Pools,\u201d","volume":"vol. 3","author":"Arlt","year":"1999"},{"issue":"5","key":"2025031810193074200_i0010-9312-70-10-1052-b19","doi-asserted-by":"crossref","first-page":"273","DOI":"10.1002\/(SICI)1521-4176(199905)50:5<273::AID-MACO273>3.0.CO;2-4","volume":"50","author":"Mietz","year":"1999","journal-title":"Mater. Corros"},{"issue":"6","key":"2025031810193074200_i0010-9312-70-10-1052-b20","doi-asserted-by":"crossref","first-page":"1431","DOI":"10.2320\/matertrans.MRA2006367","volume":"48","author":"Tani","year":"2007","journal-title":"Mater. Trans"},{"key":"2025031810193074200_i0010-9312-70-10-1052-b21","doi-asserted-by":"crossref","first-page":"42","DOI":"10.1016\/j.jnucmat.2008.06.005","volume":"379","author":"Tani","year":"2008","journal-title":"J. Nucl. Mater"},{"issue":"2","key":"2025031810193074200_i0010-9312-70-10-1052-b22","doi-asserted-by":"crossref","first-page":"105","DOI":"10.5006\/1.3319115","volume":"65","author":"Prosek","year":"2009","journal-title":"Corrosion"},{"key":"2025031810193074200_i0010-9312-70-10-1052-b23","doi-asserted-by":"crossref","DOI":"10.5006\/C2008-08484","article-title":"\u201cLow Temperature Stress Corrosion Cracking of Stainless Steels in the Atmosphere in Presence of Chloride Deposits,\u201d","author":"Prosek","year":"2008"},{"issue":"37","key":"2025031810193074200_i0010-9312-70-10-1052-b24","doi-asserted-by":"crossref","first-page":"119","DOI":"10.1149\/1.3407553","volume":"25","author":"Cook","year":"2010","journal-title":"ECS Trans"},{"issue":"10","key":"2025031810193074200_i0010-9312-70-10-1052-b25","doi-asserted-by":"crossref","first-page":"526","DOI":"10.1002\/srin.199301566","volume":"64","author":"Arlt","year":"1993","journal-title":"Steel Res"},{"key":"2025031810193074200_i0010-9312-70-10-1052-b26","doi-asserted-by":"crossref","DOI":"10.5006\/C2008-08485","article-title":"\u201cStress-Corrosion Crack Initiation of Type 304 Stainless Steel in Atmospheric Environments Containing Chloride: Influence of Surface Condition, Relative Humidity, Temperature and Thermal Sensitization,\u201d","author":"Fairweather","year":"2008"},{"key":"2025031810193074200_i0010-9312-70-10-1052-b27","first-page":"1075","volume":"49","author":"Oshikawa","year":"2000","journal-title":"Boshoku Gijutsu"},{"key":"2025031810193074200_i0010-9312-70-10-1052-b28","article-title":"\u201cStandard Practice for Determining the Inclusion or Second-Phase Constituent Content of Metals by Automatic Image Analysis\u201d","author":"ASTM E1245-03, 2008","year":"2003"},{"key":"2025031810193074200_i0010-9312-70-10-1052-b29","article-title":"\u201cStandard Practice for Assessing the Degree of Banding or Orientation of Microstructures\u201d","author":"ASTM E1268-01","year":"2007"},{"key":"2025031810193074200_i0010-9312-70-10-1052-b30","article-title":"\u201cStandard Test Methods for Determining Average Grain Size\u201d","author":"ASTM E112-96","year":"2004"},{"key":"2025031810193074200_i0010-9312-70-10-1052-b31","article-title":"\u201cStandard Test Method for Electrochemical Critical Pitting Temperature Testing of Stainless Steels\u201d","author":"ASTM G150-99","year":"2010"},{"key":"2025031810193074200_i0010-9312-70-10-1052-b32","article-title":"\u201cNon-Destructive Testing \u2013 Test Method for Residual Stress Analysis by X-Ray Diffraction\u201d","author":"EN 15305:2008","year":"2008"},{"key":"2025031810193074200_i0010-9312-70-10-1052-b33","unstructured":"M. Wanielista , R.Kersten, R.Eaglin, Hydrology Water Quantity and Quality Control, 2nd ed. (New York, NY: John Wiley & Sons, 1997)."},{"key":"2025031810193074200_i0010-9312-70-10-1052-b34","doi-asserted-by":"crossref","DOI":"10.1533\/9780857094018.166","article-title":"\u201cMetallurgical Influences on Stress Corrosion Cracking,\u201d","author":"Mureleedharan","year":"2002","journal-title":"Corrosion of Austenitic Stainless Steels: Mechanism, Mitigation and Monitoring"}],"container-title":["Corrosion"],"original-title":[],"language":"en","link":[{"URL":"https:\/\/content.ampp.org\/corrosion\/article-pdf\/70\/10\/1052\/647130\/1242.pdf","content-type":"application\/pdf","content-version":"vor","intended-application":"syndication"},{"URL":"https:\/\/content.ampp.org\/corrosion\/article-pdf\/70\/10\/1052\/647130\/1242.pdf","content-type":"unspecified","content-version":"vor","intended-application":"similarity-checking"}],"deposited":{"date-parts":[[2025,5,3]],"date-time":"2025-05-03T10:31:23Z","timestamp":1746268283000},"score":1,"resource":{"primary":{"URL":"https:\/\/content.ampp.org\/corrosion\/article\/70\/10\/1052\/1447\/Low-Temperature-Stress-Corrosion-Cracking-of"}},"subtitle":[],"short-title":[],"issued":{"date-parts":[[2014,6,16]]},"references-count":34,"journal-issue":{"issue":"10","published-print":{"date-parts":[[2014,10,1]]}},"URL":"https:\/\/doi.org\/10.5006\/1242","relation":{},"ISSN":["1938-159X","0010-9312"],"issn-type":[{"value":"1938-159X","type":"electronic"},{"value":"0010-9312","type":"print"}],"subject":[],"published":{"date-parts":[[2014,6,16]]}}}